EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

A Study on the Effects of Deep Eutectic Solvent (Chcl-Eg) Pretreatment on the Mechanical and Dimensional Stability Properties of Densified Chinese Fir

Yun Qian, Shiyu Liu, Yalan Qian, Yunyan Peng, Wenbo Che, Haili Chen, Youming Yu, Wei Zheng

Materials · 20.08.2026 · 19 (16) · 3527

DOI: 10.3390/ma19163527 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 20.08.2026. Verfasst von Yun Qian und 7 weiteren Autor:innen. Beteiligte Einrichtung: College of Chemistry and Materials Engineering, Zhejiang A&F University, Hangzhou 311300, China. Die Arbeit nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Hot-pressing densification is an effective method to improve the physical and mechanical properties of fast-growing wood, but it typically faces challenges such as moisture-induced rebound and brittle fracture of cell walls. This work proposed a strategy for preparing densified Chinese fir (DCF) via deep eutectic solvent (DES) pretreatment. The effects of pretreatment conditions (i.e., DES concentration, treatment temperature, and treatment time) and physical compression ratio on the dimensional stability, mechanical properties, and microstructure of DCF were systematically investigated. The results demonstrated that under the best-performing conditions within the investigated range conditions (10 wt% DES concentration, treatment at 100 °C for 8 h, and 50% compression ratio), the modified fir (viz., DCF) exhibited substantial improvements compared to NW in terms of modulus of rupture (147.8 MPa, a 163.5% increase), modulus of elasticity (8622 MPa, a 71.1% increase), compressive strength along the grain (81.8 MPa, a 138.5% increase), and Shore D hardness (70.6, an increase of 83.9%). Furthermore, the moisture-induced rebound rate was reduced to 0.77%, indicating that the dimensional stability of DCF was effectively enhanced. Microstructural and chemical characterization revealed that DES partially degraded part of the amorphous hemicelluloses, thereby plasticizing the cell wall and enabling cells to undergo flexible folding and dense closure during the hot-pressing process while largely retaining the main cellulose crystalline skeleton. The present work provides a feasible route for converting fast-growing plantation wood into structural materials.

Schlagwörter

Stichwörter der Autor:innen

Chinese firdeep eutectic solventdimensional stabilitymechanical propertieswood densification

Autor:innen und Institutionen

  • College of Chemistry and Materials Engineering, Zhejiang A&F University, Hangzhou 311300, China.
  • Jiyang College, Zhejiang Agriculture and Forestry University, Zhuji 311800, China.

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Qian, Y., Liu, S., Qian, Y., Peng, Y., Che, W., Chen, H., Yu, Y., & Zheng, W. (2026). A Study on the Effects of Deep Eutectic Solvent (Chcl-Eg) Pretreatment on the Mechanical and Dimensional Stability Properties of Densified Chinese Fir. Materials, 19(16), 3527. https://doi.org/10.3390/ma19163527

Vancouver

Qian Y, Liu S, Qian Y, Peng Y, Che W, Chen H, et al. A Study on the Effects of Deep Eutectic Solvent (Chcl-Eg) Pretreatment on the Mechanical and Dimensional Stability Properties of Densified Chinese Fir. Materials. 2026;19(16):3527. doi:10.3390/ma19163527

BibTeX
@article{Qian2026,
  author = {Qian, Yun and Liu, Shiyu and Qian, Yalan and Peng, Yunyan and Che, Wenbo and Chen, Haili and Yu, Youming and Zheng, Wei},
  title = {A Study on the Effects of Deep Eutectic Solvent (Chcl-Eg) Pretreatment on the Mechanical and Dimensional Stability Properties of Densified Chinese Fir},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {16},
  pages = {3527},
  doi = {10.3390/ma19163527}
}
Kostenlos starten →