EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Decoupled Mechanical and Surface Deterioration Trajectories of Cement Mortars with Different Fine Aggregates Under Freeze–Thaw Exposure

Feng Ji, Yuexiang Xing iD, Hengxuan Qiao, Jiaerheng Adelieti, Ziwei Yan, Gang Wang iD

Materials · 18.08.2026 · 19 (16) · 3480

DOI: 10.3390/ma19163480 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 18.08.2026. Verfasst von Feng Ji und 5 weiteren Autor:innen. Beteiligte Einrichtung: School of Mathematics and Physics, Xinjiang Institute of Engineering, Urumqi 830023, China. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 34 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Xinjiang Talent Development Fund, Key Laboratory Project of the Ministry of Education.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Fine-aggregate source can alter both the load-bearing response and surface scaling of mortar under freezing and thawing, but these responses are often reduced to a single durability ranking. This study compared coal gangue sand mortar (CGM), river sand mortar (RSM), desert sand mortar (DSM), and standard sand mortar (StSM) after 0, 25, and 50 freeze–thaw cycles (FTCs). Compressive strength and mass loss were measured using three replicate specimens per quantitative condition, while post-compression fragments were examined by scanning electron microscopy (SEM). The primary integrative analysis was a parameter-free two-dimensional damage-trajectory map that retained absolute compressive strength and mass loss as separate measured axes; a weighted coupled index was retained only as an auxiliary sensitivity check. Before cycling, the compressive strengths of StSM, RSM, DSM, and CGM were 68.13±0.48, 53.90±0.39, 19.47±0.33, and 6.49±0.07 MPa, respectively. After 50 FTCs, StSM retained the highest absolute strength (33.61±0.39 MPa) and the lowest mass loss (0.21±0.02%), whereas DSM retained 9.91±0.19 MPa and exhibited the highest mass loss (17.46±0.05%). The StSM trajectory moved primarily toward lower strength with negligible surface-material loss, while DSM moved toward both low residual strength and severe scaling. RSM showed substantial strength reduction followed by later-stage surface loss. CGM followed an atypical trajectory in which measured strength increased to 11.13±0.13 MPa while mass loss reached 9.67±0.04%; because age-matched non-frozen controls were unavailable, this apparent gain cannot be separated from continued hydration and specimen-age effects. The SEM images suggested pores, interfacial discontinuities, cracking, and matrix loosening, although some defects may have been induced or widened by compression. The trajectory representation exposed distinct deterioration modes without arbitrary weighting, whereas the calculated ordering of CGM and RSM in the auxiliary index changed with weighting and normalization choices. The results support reporting absolute residual strength and surface loss jointly when screening alternative fine aggregates for cold-region mortar.

Schlagwörter

Stichwörter der Autor:innen

alternative fine aggregatecement mortarcompressive strengthdamage trajectoryfreeze–thaw exposuremass lossscanning electron microscopy

Autor:innen und Institutionen

  • School of Mathematics and Physics, Xinjiang Institute of Engineering, Urumqi 830023, China.
  • Key Laboratory of Xinjiang Coal Resources Green Mining, Ministry of Education, Xinjiang Institute of Engineering, Urumqi 830023, China.
  • Xinjiang Zhongxin Construction Engineering Quality Testing Co., Ltd., Artux City 845350, China.
  • Emergency Management Science Research Institute of Xinjiang Uygur Autonomous Region, Urumqi 830011, China.
  • School of Energy Engineering, Xinjiang Institute of Engineering, Urumqi 830023, China.

ORCID-Profile: Yuexiang Xing, Gang Wang

Förderung

  • Xinjiang Talent Development Fund
  • Key Laboratory Project of the Ministry of Education

Zitieren

APA

Ji, F., Xing, Y., Qiao, H., Adelieti, J., Yan, Z., & Wang, G. (2026). Decoupled Mechanical and Surface Deterioration Trajectories of Cement Mortars with Different Fine Aggregates Under Freeze–Thaw Exposure. Materials, 19(16), 3480. https://doi.org/10.3390/ma19163480

Vancouver

Ji F, Xing Y, Qiao H, Adelieti J, Yan Z, Wang G. Decoupled Mechanical and Surface Deterioration Trajectories of Cement Mortars with Different Fine Aggregates Under Freeze–Thaw Exposure. Materials. 2026;19(16):3480. doi:10.3390/ma19163480

BibTeX
@article{Ji2026,
  author = {Ji, Feng and Xing, Yuexiang and Qiao, Hengxuan and Adelieti, Jiaerheng and Yan, Ziwei and Wang, Gang},
  title = {Decoupled Mechanical and Surface Deterioration Trajectories of Cement Mortars with Different Fine Aggregates Under Freeze–Thaw Exposure},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {16},
  pages = {3480},
  doi = {10.3390/ma19163480}
}
Kostenlos starten →