Degradation of Hydrophobic Recycled Fine Aggregate Concrete Under Chloride Salt Dry–Wet Cycling Environment

Yuwei Lu, Chunhong Chen iD, Xiaolin Zhang, Jianlei Liang, Xiang Guo iD

Materials · 17.08.2026 · 19 (16) · 3469

DOI: 10.3390/ma19163469 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 17.08.2026. Verfasst von Yuwei Lu und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Urban Construction, Changzhou University, Changzhou 213164, China. Die Arbeit nennt 99 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Reinforced concrete structures in marine environments are subjected to severe deterioration, particularly in tidal zones. The development of intrinsically hydrophobic concrete through internal modification provides a promising strategy to mitigate this challenge. This study employed sodium methyl silicate (SMS) as a hydrophobic agent to prepare recycled fine aggregate concrete (RFAC), which was subsequently subjected to accelerated indoor chloride dry–wet cycling. The deterioration behavior of RFAC and the degradation mechanism of the SMS-induced hydrophobic film during dry–wet cycling were investigated through evaluations of mechanical performance, hydrophobicity, chloride resistance, microstructure, phase composition, pore structure, chemical bonding, and functional groups. The results show that SMS improves the hydrophobicity of RFAC but inhibits its hydration process. The optimal SMS dosage for RFAC under dry–wet cycling is 9‰, which achieves a balance between hydrophobicity enhancement and pore structure optimization. Compared with ordinary RFAC, the specimen exhibits 12.9‰ and 17.6% increases in compressive strength and RDEM, respectively, after 30 cycles, accompanied by reductions of 25.8%, 52.7%, and 80.0% in peak free chloride content, chloride erosion depth, and convection zone depth, respectively. RFAC with 9‰ SMS exhibits a denser matrix with lower porosity and fewer corrosion products. SMS enhances chloride resistance mainly by reducing water transport and chloride ion ingress through hydrophobic modification. Dry–wet cycling gradually deteriorates the SMS-induced hydrophobic film through the weakening of Si-C-related structures, while the Si-O-Si framework remains relatively stable. A quantitative correlation between the contact angle and free chloride ion content is established, and the modified Lucas–Washburn equation provides a reasonable description of chloride ion penetration depth.

Schlagwörter

Stichwörter der Autor:innen

chloride dry–wet cyclingfree chloride contenthydrophobicityrecycled fine aggregate concretesilane-based network filmsodium methyl silicate

Autor:innen und Institutionen

  • School of Urban Construction, Changzhou University, Changzhou 213164, China.

ORCID-Profile: Chunhong Chen, Xiang Guo

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Lu, Y., Chen, C., Zhang, X., Liang, J., & Guo, X. (2026). Degradation of Hydrophobic Recycled Fine Aggregate Concrete Under Chloride Salt Dry–Wet Cycling Environment. Materials, 19(16), 3469. https://doi.org/10.3390/ma19163469

Vancouver

Lu Y, Chen C, Zhang X, Liang J, Guo X. Degradation of Hydrophobic Recycled Fine Aggregate Concrete Under Chloride Salt Dry–Wet Cycling Environment. Materials. 2026;19(16):3469. doi:10.3390/ma19163469

BibTeX
@article{Lu2026,
  author = {Lu, Yuwei and Chen, Chunhong and Zhang, Xiaolin and Liang, Jianlei and Guo, Xiang},
  title = {Degradation of Hydrophobic Recycled Fine Aggregate Concrete Under Chloride Salt Dry–Wet Cycling Environment},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {16},
  pages = {3469},
  doi = {10.3390/ma19163469}
}
Kostenlos starten →