Parameter Decoupling and Standardization of an RDE Protocol for CO Tolerance Evaluation of the Alkaline Hydrogen Oxidation Reaction

Hong-Fei Xing iD, Mei-Li Wang, Hao-Ran Wu, Wei-Dong Li, Bang-An Lu iD

Materials · 14.08.2026 · 19 (16) · 3460

DOI: 10.3390/ma19163460 ↗

Kurz gefasst

Studienprotokoll in der Zeitschrift Materials, online erschienen am 14.08.2026. Verfasst von Hong-Fei Xing und 4 weiteren Autor:innen. Beteiligte Einrichtung: College of Materials Science and Engineering, Zhengzhou University, Zhengzhou 450001, China. Die Arbeit nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Henan Province, China Postdoctoral Science Foundation.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

CO poisoning remains a major challenge for hydrogen fuel cells, and rotating disk electrode (RDE) measurements are widely used for preliminary screening of CO-tolerant catalysts. However, variations in key testing parameters, including catalyst loading, CO exposure time, and linear sweep voltammetry (LSV) scan rate, can substantially affect the apparent CO tolerance response and compromise cross-study comparability. Here, Pt/C was employed as a model catalyst to systematically decouple the effects of these parameters on CO tolerance evaluation of the hydrogen oxidation reaction (HOR). Catalyst loading was identified as a critical factor: at a low Pt loading of 5 μgPt cm−2, CO adsorption caused a severe decrease in the HOR limiting current, whereas at a high loading of 40 μgPt cm−2, excess available Pt sites markedly diluted the apparent poisoning effect. Electrochemical impedance analysis further revealed distinct loading-dependent changes in interfacial charge-transfer and mass-transport processes under CO-containing conditions. In addition, prolonged CO pre-exposure increased surface poisoning and current loss, while slower LSV scanning amplified the apparent poisoning response by extending the effective CO exposure time. Based on these findings, we propose a standardized RDE evaluation principle based on low catalyst loading, sufficient CO pre-exposure, and slow potential scanning, providing a more reproducible and comparable benchmark for evaluating catalyst-dependent resistance to CO poisoning under controlled RDE conditions.

Schlagwörter

Stichwörter der Autor:innen

CO tolerancealkaline hydrogen oxidation reactioncatalyst loadingelectrochemical impedance spectroscopyrotating disk electrode

Autor:innen und Institutionen

  • College of Materials Science and Engineering, Zhengzhou University, Zhengzhou 450001, China.

ORCID-Profile: Hong-Fei Xing, Bang-An Lu

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Henan Province
  • China Postdoctoral Science Foundation

Zitieren

APA

Xing, H. F., Wang, M. L., Wu, H. R., Li, W. D., & Lu, B. A. (2026). Parameter Decoupling and Standardization of an RDE Protocol for CO Tolerance Evaluation of the Alkaline Hydrogen Oxidation Reaction. Materials, 19(16), 3460. https://doi.org/10.3390/ma19163460

Vancouver

Xing HF, Wang ML, Wu HR, Li WD, Lu BA. Parameter Decoupling and Standardization of an RDE Protocol for CO Tolerance Evaluation of the Alkaline Hydrogen Oxidation Reaction. Materials. 2026;19(16):3460. doi:10.3390/ma19163460

BibTeX
@article{Xing2026,
  author = {Xing, Hong-Fei and Wang, Mei-Li and Wu, Hao-Ran and Li, Wei-Dong and Lu, Bang-An},
  title = {Parameter Decoupling and Standardization of an RDE Protocol for CO Tolerance Evaluation of the Alkaline Hydrogen Oxidation Reaction},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {16},
  pages = {3460},
  doi = {10.3390/ma19163460}
}
Kostenlos starten →