EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Macro- and Micro-Galvanic Corrosion Mechanisms in Symmetric and Asymmetric Double-Sided Friction Stir-Welded 7A65 Aluminum Alloy Joints

Chen Chen, Yichao Zhu, Zhiping He, Yanfei Wang, Weifeng Xu, Chenyang Qiu, Zhennan Liu

Materials · 04.08.2026 · 19 (15) · 3314

DOI: 10.3390/ma19153314 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 04.08.2026. Verfasst von Chen Chen und 6 weiteren Autor:innen. Beteiligte Einrichtung: China Helicopter Research and Development Institute, Jingdezhen 333001, China. Die Arbeit nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The corrosion behavior of symmetric (S-joint) and asymmetric (A-joint) double-sided friction stir-welded (DS-FSW) 7A65 aluminum alloy thick plates was investigated in 3.5 wt% NaCl solution. The S-joint, produced using the same large tool (Φ30 mm) for both passes, imposes two high-heat thermal cycles that result in insufficiently fragmented intermetallic particles (IMPs), coarse grains, and severely overaged heat-affected zones (HAZs). In contrast, the A-joint, employing a smaller tool (Φ24 mm) for the second pass, reduces the total heat input and achieves a refined microstructure with fine (2–3 µm), rounded IMPs in the second-pass weld nugget (WNZ-S) and less degraded HAZs. Electrochemical measurements reveal that the HAZ-Overlap (HAZ-O) is the most anodic zone in both joints. The S-joint shows a larger potential spread (up to ~120 mV) and higher corrosion current density than the A-joint. The hierarchical galvanic coupling, where macro-galvanic corrosion between the anodic HAZ-O and cathodic WNZs drives severe localized attack, while micro-galvanic corrosion around coarse IMPs initiates trenching, is elucidated. The A-joint mitigates this damage due to its reduced galvanic driving force (smaller potential spread of ~74 mV) and improved microstructural homogeneity. The enhanced corrosion resistance of the A-joint is attributed to grain refinement, effective IMP fragmentation, and a less degraded HAZ microstructure.

Schlagwörter

Stichwörter der Autor:innen

Al-Zn-Mg-Cu alloycorrosiondouble-sided friction stir weldingmicrostructure

Autor:innen und Institutionen

  • China Helicopter Research and Development Institute, Jingdezhen 333001, China.
  • School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China.

Zitieren

APA

Chen, C., Zhu, Y., He, Z., Wang, Y., Xu, W., Qiu, C., & Liu, Z. (2026). Macro- and Micro-Galvanic Corrosion Mechanisms in Symmetric and Asymmetric Double-Sided Friction Stir-Welded 7A65 Aluminum Alloy Joints. Materials, 19(15), 3314. https://doi.org/10.3390/ma19153314

Vancouver

Chen C, Zhu Y, He Z, Wang Y, Xu W, Qiu C, et al. Macro- and Micro-Galvanic Corrosion Mechanisms in Symmetric and Asymmetric Double-Sided Friction Stir-Welded 7A65 Aluminum Alloy Joints. Materials. 2026;19(15):3314. doi:10.3390/ma19153314

BibTeX
@article{Chen2026,
  author = {Chen, Chen and Zhu, Yichao and He, Zhiping and Wang, Yanfei and Xu, Weifeng and Qiu, Chenyang and Liu, Zhennan},
  title = {Macro- and Micro-Galvanic Corrosion Mechanisms in Symmetric and Asymmetric Double-Sided Friction Stir-Welded 7A65 Aluminum Alloy Joints},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {15},
  pages = {3314},
  doi = {10.3390/ma19153314}
}
Kostenlos starten →