EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded T-Lap Joints Between AA5083 and AA7020

Janusz Torzewski iD, Tomasz Helt, Robert Kosturek iD, Michal Jambor iD, Michal Černý, Janusz Mierzyński iD, Marcin Wachowski iD

Materials · 03.08.2026 · 19 (15) · 3286

DOI: 10.3390/ma19153286 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 03.08.2026. Verfasst von Janusz Torzewski und 6 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Mechanical Engineering, Military University of Technology, gen. S. Kaliskiego 2 Str., 00-908 Warsaw, Poland. Die Arbeit nennt 37 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Military University of Technology.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This paper investigates the microstructural evolution and mechanical performance of dissimilar friction stir-welded (FSW) T-joints produced from AA5083-H111 and AA7020-T651 aluminium alloys. The study focuses on the effects of tool rotational speed, traverse speed, and tool pin length on joint quality and mechanical strength. Welding experiments were conducted at two rotational speeds (400 and 700 rpm) and three traverse speeds (50, 100, and 200 mm/min) using two Triflute tools with pin lengths of 4.8 mm and 6.8 mm. The welded joints were examined by macro- and microstructural observations, microhardness measurements, and bending tests performed under pull-out loading conditions. The results showed that the use of the longer pin significantly improved material mixing and reduced the extent of internal defects, resulting in higher bending strength. Increasing the traverse speed improved the mechanical performance, whereas an excessively high rotational speed reduced joint strength due to increased heat input and unfavourable microstructural changes. Microhardness profiles showed no reduction in hardness within the heat-affected zones relative to the base materials and indicated localised hardening in the stir zone. For the investigated material configuration and tool geometries, the highest joint strength was obtained at a rotational speed of 400 rpm and a traverse speed of 200 mm/min using the longer-pin tool. The study confirms the critical role of process parameter optimisation and tool geometry in producing high-quality dissimilar FSW T-joints suitable for lightweight structural applications.

Schlagwörter

Stichwörter der Autor:innen

T-jointsdissimilar alloys joiningfriction stir weldingmicrostructure

Autor:innen und Institutionen

  • Faculty of Mechanical Engineering, Military University of Technology, gen. S. Kaliskiego 2 Str., 00-908 Warsaw, Poland.
  • Institute of Physics of Materials, Czech Academy of Sciences, Žižkova 513/22, 61600 Brno, Czech Republic.

ORCID-Profile: Janusz Torzewski, Robert Kosturek, Michal Jambor, Janusz Mierzyński, Marcin Wachowski

Förderung

  • Military University of Technology

Zitieren

APA

Torzewski, J., Helt, T., Kosturek, R., Jambor, M., Černý, M., Mierzyński, J., & Wachowski, M. (2026). Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded T-Lap Joints Between AA5083 and AA7020. Materials, 19(15), 3286. https://doi.org/10.3390/ma19153286

Vancouver

Torzewski J, Helt T, Kosturek R, Jambor M, Černý M, Mierzyński J, et al. Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded T-Lap Joints Between AA5083 and AA7020. Materials. 2026;19(15):3286. doi:10.3390/ma19153286

BibTeX
@article{Torzewski2026,
  author = {Torzewski, Janusz and Helt, Tomasz and Kosturek, Robert and Jambor, Michal and Černý, Michal and Mierzyński, Janusz and Wachowski, Marcin},
  title = {Microstructure and Mechanical Properties of Dissimilar Friction Stir Welded T-Lap Joints Between AA5083 and AA7020},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {15},
  pages = {3286},
  doi = {10.3390/ma19153286}
}
Kostenlos starten →