EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Interfacial Microstructure Evolution and High-Speed Ball Shear Fracture of SAC305/Cu-20wt%Zn Solder Joints Under Isothermal Aging

Jae-Yong Park, Sehoon Yoo iD

Materials · 22.07.2026 · 19 (14) · 3138

DOI: 10.3390/ma19143138 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 22.07.2026. Verfasst von Jae-Yong Park und 1 weiteren Autor:innen. Beteiligte Einrichtung: Division of Materials Science & Engineering, Hanyang University, Seoul 133-791, Republic of Korea. Die Arbeit nennt 26 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Ministry of Trade, Industry and Energy.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The interfacial microstructure evolution and high-speed ball shear reliability of SAC305 (Sn-3.0Ag-0.5Cu)/Cu-20wt%Zn solder joints were systematically investigated after isothermal aging at 180 °C for up to 250 h. SAC305/electroless nickel immersion gold (ENIG) joints were used as a comparative reference. Unlike prior studies that benchmarked Cu-Zn against bare Cu, this work directly compares the two systems, establishing ENIG as the industrially relevant reference. Cu6(Sn,Zn)5 was identified as the dominant intermetallic compound (IMC) phase at the SAC305/Cu-Zn interface by SEM/EDS analysis. At the SAC305/ENIG interface, (Cu,Ni)6Sn5 formed as the dominant IMC phase, accompanied by a P-rich layer at the (Cu,Ni)6Sn5/Ni(P) boundary. The IMC thickness of SAC305/Cu-Zn joints increased from approximately 2.50 μm in the as-reflowed condition to 3.41 μm at 250 h, consistently exceeding that of SAC305/ENIG joints (1.94–2.25 μm) throughout aging. Despite this, the high-speed ball shear strength of SAC305/Cu-Zn joints was equivalent or superior to that of SAC305/ENIG joints at all aging durations. Fractographic analysis confirmed that the P-rich layer in ENIG joints acted as a preferential crack propagation path under impact loading, driving the brittle fracture ratio to approximately 75% at 250 h—compared to approximately 47% in SAC305/Cu-Zn joints. These results demonstrate that Cu-Zn electroplated from a neutral pyrophosphate-based bath constitutes a highly reliable wetting layer, offering impact reliability equivalent or superior to that of the conventional ENIG surface finish.

Schlagwörter

Stichwörter der Autor:innen

Cu-Zn layerSn-Ag-Cu solderelectroless Ni immersion goldhigh-speed shear testintermetallic compoundshear strength

Autor:innen und Institutionen

  • Division of Materials Science & Engineering, Hanyang University, Seoul 133-791, Republic of Korea.
  • Advanced Packaging Integration Center (APIC), Korea Institute of Industrial Technology, Incheon 406-840, Republic of Korea.

ORCID-Profile: Sehoon Yoo

Förderung

  • Ministry of Trade, Industry and Energy

Zitieren

APA

Park, J. Y., & Yoo, S. (2026). Interfacial Microstructure Evolution and High-Speed Ball Shear Fracture of SAC305/Cu-20wt%Zn Solder Joints Under Isothermal Aging. Materials, 19(14), 3138. https://doi.org/10.3390/ma19143138

Vancouver

Park JY, Yoo S. Interfacial Microstructure Evolution and High-Speed Ball Shear Fracture of SAC305/Cu-20wt%Zn Solder Joints Under Isothermal Aging. Materials. 2026;19(14):3138. doi:10.3390/ma19143138

BibTeX
@article{Park2026,
  author = {Park, Jae-Yong and Yoo, Sehoon},
  title = {Interfacial Microstructure Evolution and High-Speed Ball Shear Fracture of SAC305/Cu-20wt%Zn Solder Joints Under Isothermal Aging},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {14},
  pages = {3138},
  doi = {10.3390/ma19143138}
}
Kostenlos starten →