EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Densification and Mechanical Properties of Monolithic B4C and In-Situ Formed TiB2 Containing B4C–TiB2: Effects of Particle Size and Impurity

İlker Solakoğlu iD, Furkan Buluç iD, Bahadır Tunaboylu iD, Servet Turan

Materials · 02.07.2026 · 19 (13) · 2820

DOI: 10.3390/ma19132820 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 02.07.2026. Verfasst von İlker Solakoğlu und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Metallurgical and Materials Engineering, Faculty of Engineering, Marmara University, 34854 Istanbul, Türkiye. Die Arbeit nennt 37 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: TRBOR Boron Technologies Inc, TRBOR Boron Technologies Inc..

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the effects of particle size, powder purity, and in situ TiB2 formation on the densification behavior and mechanical properties of B4C-based ceramics fabricated via spark plasma sintering (SPS). The results demonstrate that particle size is the dominant parameter controlling densification and microstructural evolution. An intermediate particle size (F1200) yields the highest relative density (98.41%) and superior mechanical properties, including a hardness of 33.34 GPa and fracture toughness of 4.63 MPa·m1/2, by providing an optimal balance between diffusion kinetics and particle packing. The in situ formed TiB2 significantly enhances fracture toughness compared to monolithic B4C. Among the composite samples, the medium particle size containing BT1200 exhibits the best overall combination of properties, with a relative density of 98.00%, hardness of 25.40 GPa, and fracture toughness of 5.18 MPa·m1/2. The highest fracture toughness is achieved in the largest particle size containing BT325 (6.29 MPa·m1/2), confirming the effectiveness of TiB2 combined with large particle size as a toughening phase. Although higher powder purity contributes to improved phase homogeneity, its influence on densification and mechanical performance is secondary compared to particle size and pore evolution. Excessive particle refinement leads to residual porosity, limiting full densification. Overall, optimizing particle size together with controlled in situ TiB2 formation is essential for achieving high-performance B4C-based ceramics and composites. These findings provide a practical framework for tailoring microstructure and mechanical properties in advanced ultra-hard ceramic systems.

Schlagwörter

Stichwörter der Autor:innen

boron carbide (B4C)mechanical propertiesmicrostructureparticle sizepurityspark plasma sintering (SPS)titanium carbide (TiC)

Autor:innen und Institutionen

  • Department of Metallurgical and Materials Engineering, Faculty of Engineering, Marmara University, 34854 Istanbul, Türkiye.
  • TRBOR Boron Technologies Inc., 34906 Istanbul, Türkiye.
  • Ceramic Research Center, 26005 Eskişehir, Türkiye.
  • Deputy Vice Chancellor Office of Graduate Research, Sultan Qaboos University, Al Khoud, Muscat P.O. Box 17, Oman.
  • Department of Materials Science and Engineering, Faculty of Engineering, Eskisehir Technical University, 26555 Eskişehir, Türkiye.

ORCID-Profile: İlker Solakoğlu, Furkan Buluç, Bahadır Tunaboylu

Förderung

  • TRBOR Boron Technologies Inc
  • TRBOR Boron Technologies Inc.

Zitieren

APA

Solakoğlu, İ., Buluç, F., Tunaboylu, B., & Turan, S. (2026). Densification and Mechanical Properties of Monolithic B4C and In-Situ Formed TiB2 Containing B4C–TiB2: Effects of Particle Size and Impurity. Materials, 19(13), 2820. https://doi.org/10.3390/ma19132820

Vancouver

Solakoğlu İ, Buluç F, Tunaboylu B, Turan S. Densification and Mechanical Properties of Monolithic B4C and In-Situ Formed TiB2 Containing B4C–TiB2: Effects of Particle Size and Impurity. Materials. 2026;19(13):2820. doi:10.3390/ma19132820

BibTeX
@article{Solakolu2026,
  author = {Solakoğlu, İlker and Buluç, Furkan and Tunaboylu, Bahadır and Turan, Servet},
  title = {Densification and Mechanical Properties of Monolithic B4C and In-Situ Formed TiB2 Containing B4C–TiB2: Effects of Particle Size and Impurity},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {13},
  pages = {2820},
  doi = {10.3390/ma19132820}
}
Kostenlos starten →