EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Analysis of Al2O3 Single-Bead Deposition Behavior and Microstructure on a Ti-6Al-4V Substrate Using the Laser-Directed Energy Deposition (DED-LB) Process

Tae-Hyeon Kim, Jin-Soo Lee iD, Sang-In Kim, Su-Han Bae, Changjong Kim iD, Se-Yun Kim iD

Materials · 02.06.2026 · 19 (11) · 2369

DOI: 10.3390/ma19112369 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 02.06.2026. Verfasst von Tae-Hyeon Kim und 5 weiteren Autor:innen. Beteiligte Einrichtung: Department of Mechatronics Engineering, Kyungnam University, Changwon 51767, Republic of Korea. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Korea AeroSpace Administration, Ministry of Education.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Al2O3 single beads were deposited on a Ti-6Al-4V (Ti64) substrate by laser-directed energy deposition (DED-LB) to establish baseline process conditions for ceramic protective layers and future Ti64/Al2O3 functionally graded materials (FGMs). These ceramic-containing surface layers are applicable to titanium components requiring improved oxidation, wear, and thermal resistance in aerospace, automotive, and high-temperature structural applications. Laser power (300–700 W) and scan speed (300–700 mm/min) were varied, and bead geometry was quantified from cross-sectional observations; energy density and dilution ratio were calculated. Melt pool depth increased with higher power and lower speed, indicating increased heat input and substrate melting. Crack formation in the melt zone was more sensitive to laser power than to scan speed. In contrast, bead height showed a non-monotonic response to energy density, which may be associated with possible coupled effects such as recoil pressure-driven melt pool disturbance, powder scattering, and insufficient powder melting at high scan speeds. Dilution-based optimization identified 300 W laser power and 400 mm/min scan speed, with a powder feed rate of 3 g/min, as the most suitable condition within the investigated process window, giving the lowest practical dilution ratio of approximately 40.27%. SEM–EDS and XRD analyses were conducted to examine the interfacial microstructure and phase characteristics under the selected condition. Overall, this study provides fundamental process guidelines and mechanistic insight into bead formation, dilution behavior, and interface formation, supporting the future application of DED-LB-based ceramic protective or graded layers on Ti64 surfaces.

Schlagwörter

Stichwörter der Autor:innen

Al2O3Ti-6Al-4V (Ti64)additive manufacturingdilution ratiolaser-directed energy deposition (DED-LB)

Autor:innen und Institutionen

  • Department of Mechatronics Engineering, Kyungnam University, Changwon 51767, Republic of Korea.
  • Digital Manufacturing Innovation Division, Research Institute of Medium & Small Shipbuilding, Busan 46757, Republic of Korea.
  • Department of Future Automotive Engineering, Kyungnam University, Changwon 51767, Republic of Korea.

ORCID-Profile: Jin-Soo Lee, Changjong Kim, Se-Yun Kim

Förderung

  • Korea AeroSpace Administration
  • Ministry of Education

Zitieren

APA

Kim, T. H., Lee, J. S., Kim, S. I., Bae, S. H., Kim, C., & Kim, S. Y. (2026). Analysis of Al2O3 Single-Bead Deposition Behavior and Microstructure on a Ti-6Al-4V Substrate Using the Laser-Directed Energy Deposition (DED-LB) Process. Materials, 19(11), 2369. https://doi.org/10.3390/ma19112369

Vancouver

Kim TH, Lee JS, Kim SI, Bae SH, Kim C, Kim SY. Analysis of Al2O3 Single-Bead Deposition Behavior and Microstructure on a Ti-6Al-4V Substrate Using the Laser-Directed Energy Deposition (DED-LB) Process. Materials. 2026;19(11):2369. doi:10.3390/ma19112369

BibTeX
@article{Kim2026,
  author = {Kim, Tae-Hyeon and Lee, Jin-Soo and Kim, Sang-In and Bae, Su-Han and Kim, Changjong and Kim, Se-Yun},
  title = {Analysis of Al2O3 Single-Bead Deposition Behavior and Microstructure on a Ti-6Al-4V Substrate Using the Laser-Directed Energy Deposition (DED-LB) Process},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {11},
  pages = {2369},
  doi = {10.3390/ma19112369}
}
Kostenlos starten →