Fabrication and Bonding Strength of Sn-Decorated MWCNT-Reinforced Sn-3.0Ag-0.5Cu Composite Solder Joints: Reflow vs. IPL Soldering
Materials · 22.05.2026 · 19 (11) · 2188
DOI: 10.3390/ma19112188 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 22.05.2026. Verfasst von DongGil Kang und 6 weiteren Autor:innen. Beteiligte Einrichtung: School of Advanced Materials Science & Engineering, Sungkyunkwan University, 2066 Seobu-ro, Jangan-gu, Suwon 16419, Republic of Korea. Die Arbeit nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Research Foundation of Korea, Ministry of Science and ICT, Korea government.
Abstract (Originalsprache)
The rapid advancement of microelectronic packaging has created a critical need for lead-free solder joints with enhanced mechanical and thermal reliability. This study introduces a novel approach to improve Sn-3.0Ag-0.5Cu (SAC 305) solder joints by incorporating Sn-decorated multiwalled carbon nanotubes (MWCNTs). To address the poor wettability and agglomeration of carbon nanotubes in molten solder, MWCNTs were functionalized and uniformly coated with ~70 nm Sn nanoparticles via electroless plating. Soldering was conducted using intense pulsed light (IPL), a rapid, energy-efficient heat source, and was compared with conventional reflow soldering. The study systematically investigated the influence of MWCNT content (0, 0.05, 0.1, and 0.2 wt.%) and IPL soldering conditions with pulse numbers: 27–36 for shear tests, and 30–42 for drop impact tests. IPL processing produced thinner Cu6Sn5 IMC layers than reflow soldering due to its shorter duration. The composite solder with 0.1 wt.% Sn-decorated MWCNTs achieved the highest density, superior thermal dissipation in LED packages, and maximum shear strength and drop impact resistance. These results demonstrate that optimizing Sn-MWCNT content, especially at 0.1 wt.%, and precisely controlling IPL energy can yield highly reliable, mechanically robust, and thermally efficient lead-free solder joints for advanced electronic packaging.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Advanced Materials Science & Engineering, Sungkyunkwan University, 2066 Seobu-ro, Jangan-gu, Suwon 16419, Republic of Korea.
- Department of Semiconductor Convergence Engineering, Sungkyunkwan University, 2066 Seobu-ro, Jangan-gu, Suwon 16419, Republic of Korea.
- School of Advanced Materials Science & Engineering, Chungbuk University, Chungdae-ro, Seowon-gu, Cheongju-si 28644, Republic of Korea.
ORCID-Profile: JeongWon Yoon
Förderung
- National Research Foundation of Korea
- Ministry of Science and ICT
- Korea government
Zitieren
APA
Kang, D., Seong, H., Yoon, J., Sung, M., Joo, J., Yoon, J., & Jung, S. (2026). Fabrication and Bonding Strength of Sn-Decorated MWCNT-Reinforced Sn-3.0Ag-0.5Cu Composite Solder Joints: Reflow vs. IPL Soldering. Materials, 19(11), 2188. https://doi.org/10.3390/ma19112188
Vancouver
Kang D, Seong H, Yoon J, Sung M, Joo J, Yoon J, et al. Fabrication and Bonding Strength of Sn-Decorated MWCNT-Reinforced Sn-3.0Ag-0.5Cu Composite Solder Joints: Reflow vs. IPL Soldering. Materials. 2026;19(11):2188. doi:10.3390/ma19112188
BibTeX
@article{Kang2026,
author = {Kang, DongGil and Seong, HoGyeong and Yoon, JaeJun and Sung, MinJae and Joo, JinHo and Yoon, JeongWon and Jung, SeungBoo},
title = {Fabrication and Bonding Strength of Sn-Decorated MWCNT-Reinforced Sn-3.0Ag-0.5Cu Composite Solder Joints: Reflow vs. IPL Soldering},
journal = {Materials},
year = {2026},
volume = {19},
number = {11},
pages = {2188},
doi = {10.3390/ma19112188}
}
EUVIMED