EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Microhardness Recovery and Micromorphology of Demineralized Dentin Restored with Modified Glass Hybrid Material

Ivan Šalinović iD, Maja Bilić-Prcić, Maria Bota, Anja Ivica, Ivana Miletić iD

Materials · 24.04.2026 · 19 (9) · 1733

DOI: 10.3390/ma19091733 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 24.04.2026. Verfasst von Ivan Šalinović und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Dental Medicine, University of Zagreb, Gundulićeva 5, 10000 Zagreb, Croatia. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Croatian Science Foundation.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study evaluated how the addition of 5 wt% bioactive glass and 15 wt% short glass fibers to EQUIA Forte HT affects the microhardness, micromorphology, and elemental composition of demineralized dentin. Class I cavities in 28 human third molars were demineralized with 37% phosphoric acid and restored with: (1) Filtek Universal composite, (2) EQUIA Forte HT, (3) EQUIA Forte HT + 5wt% BAG, or (4) EQUIA Forte HT + 15wt% short glass fibers. After 4 weeks of storage in phosphate-buffered saline at 37 °C, the teeth were cut in half, obtaining two samples from each tooth (n = 14). Vickers microhardness (HV0.1) was measured on demineralized dentin 50–100 μm apical to the restoration interface. Representative specimens (n = 2) were examined using scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). Data were analyzed with one-way ANOVA (α = 0.05). Unmodified EQUIA Forte HT showed the highest mean dentin microhardness recovery (25.06 ± 1.42 HV0.1), followed by composite (17.31 ± 0.66 HV0.1), BAG-modified (23.74 ± 1.37 HV0.1) and fiber-reinforced (22.15 ± 1.06 HV0.1) groups (p < 0.001, all pairwise comparisons p ≤ 0.039). Glass hybrids showed prominent Ca/P peaks; modified groups had elevated Si (BAG) and Al (fibers). SEM revealed smoother surfaces with fewer cracks in modified materials. Unmodified EQUIA Forte HT produced the highest short-term microhardness recovery, while BAG and fiber additions altered surface morphology and elemental composition but slightly reduced early hardness.

Schlagwörter

Stichwörter der Autor:innen

bioactive glassdentin remineralizationglass hybridsmicrohardnessshort glass fibers

Autor:innen und Institutionen

  • School of Dental Medicine, University of Zagreb, Gundulićeva 5, 10000 Zagreb, Croatia.

ORCID-Profile: Ivan Šalinović, Ivana Miletić

Förderung

  • Croatian Science Foundation

Zitieren

APA

Šalinović, I., Bilić-Prcić, M., Bota, M., Ivica, A., & Miletić, I. (2026). Microhardness Recovery and Micromorphology of Demineralized Dentin Restored with Modified Glass Hybrid Material. Materials, 19(9), 1733. https://doi.org/10.3390/ma19091733

Vancouver

Šalinović I, Bilić-Prcić M, Bota M, Ivica A, Miletić I. Microhardness Recovery and Micromorphology of Demineralized Dentin Restored with Modified Glass Hybrid Material. Materials. 2026;19(9):1733. doi:10.3390/ma19091733

BibTeX
@article{alinovi2026,
  author = {Šalinović, Ivan and Bilić-Prcić, Maja and Bota, Maria and Ivica, Anja and Miletić, Ivana},
  title = {Microhardness Recovery and Micromorphology of Demineralized Dentin Restored with Modified Glass Hybrid Material},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {9},
  pages = {1733},
  doi = {10.3390/ma19091733}
}
Kostenlos starten →