Axial–Flexural Performance of Steel Fiber-Reinforced Concrete Columns: Effects of Axial Load Ratio and Steel Fiber Volume Fraction

Sang-Woo Kim iD, In-Ho Park, Seungwook Seok, Wonchang Choi iD, Jinsup Kim

Materials · 06.03.2026 · 19 (5) · 1014

DOI: 10.3390/ma19051014 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 06.03.2026. Verfasst von Sang-Woo Kim und 4 weiteren Autor:innen. Beteiligte Einrichtung: Department of Civil Engineering, Gyeongsang National University, Jinju 52828, Republic of Korea. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Research Foundation of Korea.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the axial–flexural behavior of steel fiber–reinforced concrete (SFRC) columns under combined constant axial load and monotonic lateral loading. Nine column specimens with different axial load ratios (0.0, 0.10, and 0.20) and steel fiber contents (0.0%, 0.5%, and 1.0%) were tested under monotonic loading to evaluate their failure modes, load–deflection behavior, ductility, and energy absorption capacity. In addition, a sectional P–M interaction analysis was performed to examine the influence of steel fiber inclusion on flexural strength under different axial compression levels. The interaction diagrams indicated that steel fibers expanded the flexural strength envelope, with a more pronounced enhancement in the low-axial-load region. The test results revealed that increasing the axial load ratio enhanced the specimens’ peak load capacity but reduced their ductility, leading to a brittle failure mode. Conversely, the incorporation of steel fiber improved the crack distribution, delayed crack propagation, and enhanced both ductility and energy absorption, particularly under moderate axial load conditions. The failure modes were characterized generally by flexural cracking and localized crushing in the compression zone, with the specimens that contained steel fiber exhibiting a more gradual post-peak load response than the specimens without steel fiber. The energy absorption capacity, quantified as the area under the load–deflection curve, was maximized when the axial load ratio of 0.10 was used in tandem with steel fiber reinforcement, indicating an optimal balance between strength and ductility. Overall, steel fiber inclusion improved deformation capacity and energy absorption under monotonic loading, particularly at low-to-moderate axial load ratios.

Schlagwörter

Stichwörter der Autor:innen

axial load ratioflexural behaviormonotonic loadingreinforced concrete columnsteel fiber

Autor:innen und Institutionen

  • Department of Civil Engineering, Gyeongsang National University, Jinju 52828, Republic of Korea.
  • Department of Architectural Engineering, Gachon University, Seongnam-si 13120, Republic of Korea.

ORCID-Profile: Sang-Woo Kim, Wonchang Choi

Förderung

  • National Research Foundation of Korea

Zitieren

APA

Kim, S. W., Park, I. H., Seok, S., Choi, W., & Kim, J. (2026). Axial–Flexural Performance of Steel Fiber-Reinforced Concrete Columns: Effects of Axial Load Ratio and Steel Fiber Volume Fraction. Materials, 19(5), 1014. https://doi.org/10.3390/ma19051014

Vancouver

Kim SW, Park IH, Seok S, Choi W, Kim J. Axial–Flexural Performance of Steel Fiber-Reinforced Concrete Columns: Effects of Axial Load Ratio and Steel Fiber Volume Fraction. Materials. 2026;19(5):1014. doi:10.3390/ma19051014

BibTeX
@article{Kim2026,
  author = {Kim, Sang-Woo and Park, In-Ho and Seok, Seungwook and Choi, Wonchang and Kim, Jinsup},
  title = {Axial–Flexural Performance of Steel Fiber-Reinforced Concrete Columns: Effects of Axial Load Ratio and Steel Fiber Volume Fraction},
  journal = {Materials},
  year = {2026},
  volume = {19},
  number = {5},
  pages = {1014},
  doi = {10.3390/ma19051014}
}
Kostenlos starten →