EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Effect of Mn Content and Heat Treatment on Microstructure and Properties of Laser Cladding of FeCoNiCrTi High-Entropy Alloy Coating

Shibang Ma iD, Yicheng Zhou, Congzheng Zhang iD, Zhengchun Xu iD, Chengguo Fu iD

Materials · 13.11.2025 · 18 (22) · 5160

DOI: 10.3390/ma18225160 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 13.11.2025. Verfasst von Shibang Ma und 4 weiteren Autor:innen. Beteiligte Einrichtung: School of Intelligent Manufacturing and Electrical Engineering, Nanyang Normal University, Nanyang 473061, China. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Henan Province science and technology research project, Joint Science and Technology Project of Bijie.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, the effects of different Mn content and heat treatment on the microstructure and properties of CoCrFeNiTi coatings by laser cladding technology were investigated. Scanning electron microscopy, energy-dispersive spectrometry, and X-ray diffraction were used to analyze the structure and composition. The hardness and wear resistance were tested by a microhardness tester and a friction-wear tester. The results show that there are many intermetallic compounds rich in Ti and Ni between the grains. As the Mn content increases, the coating gradually transitions from a dual-phase structure of BCC and FCC to a single FCC structure. The hardness of the coating decreases gradually with the increase in Mn content due to the change in the phase structure, while the friction coefficient decreases slightly at first and then increases significantly. The main wear mechanisms of the coating are adhesive wear and abrasive wear. After heat treatment at 600 °C, petal-like Laves precipitates appear. The average microhardness of CoCrFeNiTi coatings after heat treatment is lower than before treatment, and the friction coefficient is higher than before treatment. The average microhardness of the coating increases slightly with the increase in the treatment temperature. The average friction coefficient of the coating obtained after heat treatment at 600 °C is only 0.5941 because of its uniform microstructure. Therefore, it is reduced by approximately 15% compared with the base metal.

Schlagwörter

Stichwörter der Autor:innen

FeCoNiCrTiMnx coatingfriction coefficientheat treatmentlaser claddingmicrohardnessmicrostructure evolution

Autor:innen und Institutionen

  • School of Intelligent Manufacturing and Electrical Engineering, Nanyang Normal University, Nanyang 473061, China.
  • Collaborative Innovation Center of Intelligent Explosion-Proof Equipment, Henan Province, Nanyang 473061, China.
  • School of Mechanical Engineering, Guizhou University of Engineering Science, Bijie 551700, China.

ORCID-Profile: Shibang Ma, Congzheng Zhang, Zhengchun Xu, Chengguo Fu

Förderung

  • Henan Province science and technology research project
  • Joint Science and Technology Project of Bijie

Zitieren

APA

Ma, S., Zhou, Y., Zhang, C., Xu, Z., & Fu, C. (2025). Effect of Mn Content and Heat Treatment on Microstructure and Properties of Laser Cladding of FeCoNiCrTi High-Entropy Alloy Coating. Materials, 18(22), 5160. https://doi.org/10.3390/ma18225160

Vancouver

Ma S, Zhou Y, Zhang C, Xu Z, Fu C. Effect of Mn Content and Heat Treatment on Microstructure and Properties of Laser Cladding of FeCoNiCrTi High-Entropy Alloy Coating. Materials. 2025;18(22):5160. doi:10.3390/ma18225160

BibTeX
@article{Ma2025,
  author = {Ma, Shibang and Zhou, Yicheng and Zhang, Congzheng and Xu, Zhengchun and Fu, Chengguo},
  title = {Effect of Mn Content and Heat Treatment on Microstructure and Properties of Laser Cladding of FeCoNiCrTi High-Entropy Alloy Coating},
  journal = {Materials},
  year = {2025},
  volume = {18},
  number = {22},
  pages = {5160},
  doi = {10.3390/ma18225160}
}
Kostenlos starten →