Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 06.11.2025. Verfasst von Liuxu Cao und 3 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: The Special Funds of the National Natural Science Foundation of China, Special Funds of the National Natural Science Foundation of China, National Natural Science Foundation of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Compared to pure aluminum powder, aluminum alloy powders exhibit higher strength and hardness, which leads to greater difficulty in plastic deformation during cold compaction, consequently impairing green compact formation and subsequent densification. This study introduces pure aluminum powder into the raw material system based on 2024 aluminum alloy powder and SiC powder, effectively improving the powder compaction characteristics. A systematic investigation was conducted to examine the effects of sintering temperature (460–640 °C) and holding time (5–120 min) during pressureless sintering on the sintering shrinkage, relative density, mechanical properties, and microstructure of SiCp/Al composites reinforced with 35 wt.% of 31.9 μm SiC particles. The results indicate that sintering at 600 °C for 30 min constitutes the optimal process condition, achieving effective interparticle bonding while preventing coarsening of both precipitates and pores. Subsequent hot pressing effectively enhanced the relative density and mechanical properties of the sintered preforms, achieving a maximum tensile strength of 343 MPa, which represents an improvement of over 70% compared to the sintered-only state. For the hot-pressed state, elevated levels of SiC particle content and size compromised its mechanical performance. This work demonstrates a highly operable and industrially viable processing route for manufacturing aluminum matrix composites using alloy powders.

Schlagwörter

Stichwörter der Autor:innen

aluminum matrix compositesdensificationmicrostructurepowder metallurgy

Autor:innen und Institutionen

  • State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China.
  • Light Alloy Research Institute, Central South University, Changsha 410083, China.
  • School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China.

Förderung

  • The Special Funds of the National Natural Science Foundation of China
  • Special Funds of the National Natural Science Foundation of China
  • National Natural Science Foundation of China
  • Joint Fund for Regional Innovation of Hunan Provincial Natural Science Foundation

Zitieren

APA

Cao, L., Dai, Q., Liang, Q., & Zhang, X. (2025). The Influence of Process Conditions and Reinforcement Characteristics on the Densification and Mechanical Properties of Powder Metallurgy SiCp/Al Composites. Materials, 18(21), 5060. https://doi.org/10.3390/ma18215060

Vancouver

Cao L, Dai Q, Liang Q, Zhang X. The Influence of Process Conditions and Reinforcement Characteristics on the Densification and Mechanical Properties of Powder Metallurgy SiCp/Al Composites. Materials. 2025;18(21):5060. doi:10.3390/ma18215060

BibTeX
@article{Cao2025,
  author = {Cao, Liuxu and Dai, Qingsong and Liang, Qiwen and Zhang, Xiaoyong},
  title = {The Influence of Process Conditions and Reinforcement Characteristics on the Densification and Mechanical Properties of Powder Metallurgy SiCp/Al Composites},
  journal = {Materials},
  year = {2025},
  volume = {18},
  number = {21},
  pages = {5060},
  doi = {10.3390/ma18215060}
}