Shear Performance Degradation of Fiber-Reinforced Recycled Aggregate Concrete Beams Under Salt Freeze–Thaw Cycles

Shefeng Guo, Jin Wu iD, Jingmiao Zhao, Zhehong Zeng, Xiangyu Wang, Yiyuan Wang, Haoxiang Luan, Yulin Wang, Dongxia Hu

Materials · 21.10.2025 · 18 (20) · 4817

DOI: 10.3390/ma18204817 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 21.10.2025. Verfasst von Shefeng Guo und 8 weiteren Autor:innen. Beteiligte Einrichtung: College of Civil Aviation, Nanjing University of Aeronautics and Astronautics, Nanjing 211106, China. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 65 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In saline soil and alpine regions of northwest China, fiber-reinforced recycled aggregate concrete (FR-RAC) beams are subjected to coupled degradation from a chloride–sulfate composite salt attack and freeze–thaw cycling. Existing studies predominantly focus on natural aggregate concrete in freshwater environments or single-salt solutions, with limited documentation on the shear performance of FR-RAC beams after freeze–thaw exposure in chloride–sulfate composite salt solutions. To investigate the durability degradation patterns of FR-RAC beams in Xinjiang’s saline soil regions, two exposure environments (pure water and 5% NaCl + 2.0% Na2SO4 composite salt solution) were established. Shear performance tests were conducted on nine groups of FR-RAC beams after 0–175 freeze–thaw cycles, with measurements focusing on failure modes, cracking loads, and ultimate shear capacities. The results revealed that under composite salt freeze–thaw conditions: after 100 cycles, the cracking load and shear capacity of tested beams decreased by 39.8% and 22.2%, respectively, compared to unfrozen specimens representing reductions 29.6% and 82.0% greater than those in freshwater environments; at 175 cycles, cumulative damage intensified, with total reductions reaching 56.8% (cracking load) and 36.1% (shear capacity). A shear capacity degradation prediction model for FR-RAC beams under composite salt freeze–thaw coupling was developed, accounting for concrete strength attenuation and interfacial bond degradation. Model validation demonstrated excellent agreement between predicted and experimental values, confirming its robust applicability.

Schlagwörter

Stichwörter der Autor:innen

composite salt freeze-thawpolypropylene fiberrecycled aggregate concrete beamshear performance degradation

Autor:innen und Institutionen

  • College of Civil Aviation, Nanjing University of Aeronautics and Astronautics, Nanjing 211106, China.
  • Xinjiang Vocational & Technical College of Communications, Urumqi 831401, China.

ORCID-Profile: Jin Wu

Zitieren

APA

Guo, S., Wu, J., Zhao, J., Zeng, Z., Wang, X., Wang, Y., Luan, H., Wang, Y., & Hu, D. (2025). Shear Performance Degradation of Fiber-Reinforced Recycled Aggregate Concrete Beams Under Salt Freeze–Thaw Cycles. Materials, 18(20), 4817. https://doi.org/10.3390/ma18204817

Vancouver

Guo S, Wu J, Zhao J, Zeng Z, Wang X, Wang Y, et al. Shear Performance Degradation of Fiber-Reinforced Recycled Aggregate Concrete Beams Under Salt Freeze–Thaw Cycles. Materials. 2025;18(20):4817. doi:10.3390/ma18204817

BibTeX
@article{Guo2025,
  author = {Guo, Shefeng and Wu, Jin and Zhao, Jingmiao and Zeng, Zhehong and Wang, Xiangyu and Wang, Yiyuan and Luan, Haoxiang and Wang, Yulin and Hu, Dongxia},
  title = {Shear Performance Degradation of Fiber-Reinforced Recycled Aggregate Concrete Beams Under Salt Freeze–Thaw Cycles},
  journal = {Materials},
  year = {2025},
  volume = {18},
  number = {20},
  pages = {4817},
  doi = {10.3390/ma18204817}
}
Kostenlos starten →