Residual Flexural Behavior of Hybrid Fiber-Reinforced Geopolymer After High Temperature Exposure
Materials · 30.07.2025 · 18 (15) · 3572
DOI: 10.3390/ma18153572 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 30.07.2025. Verfasst von Yiyang Xiong und 3 weiteren Autor:innen. Beteiligte Einrichtung: School of Civil Engineering and Architecture, Wuhan University of Technology, Wuhan 430070, China. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Wuhan Science and Technology Bureau, Wuhan Knowledge Innovation Project.
Abstract (Originalsprache)
Cement-based building materials usually exhibit weak flexural behavior under high temperature or fire conditions. This paper develops a novel geopolymer with enhanced residual flexural strength, incorporating fly ash/metakaolin precursors and corundum aggregates based on our previous study, and further improves flexural performance using hybrid fibers. The flexural load–deflection response, strength, deformation capacity, toughness and microstructure are investigated by a thermal exposure test, bending test and microstructure observation. The results indicate that the plain geopolymer exhibits a continuously increasing flexural strength from 10 MPa at 20 °C to 25.9 MPa after 1000 °C exposure, attributed to thermally induced further geopolymerization and ceramic-like crystalline phase formation. Incorporating 5% wollastonite fibers results in slightly increased initial and residual flexural strength but comparable peak deflection, toughness and brittle failure. The binary 5% wollastonite and 1% basalt fibers in geopolymer obviously improve residual flexural strength exposed to 400–800 °C. The steel fibers show remarkable reinforcement on flexural behavior at 20–800 °C exposure; however, excessive steel fiber content such as 2% weakens flexural properties after 1000 °C exposure due to severe oxidation deterioration and thermal incompatibility. The wollastonite/basalt/steel fibers exhibit a positive synergistic effect on flexural strength and toughness of geopolymers at 20–600 °C.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Civil Engineering and Architecture, Wuhan University of Technology, Wuhan 430070, China.
ORCID-Profile: Peipeng Li
Förderung
- Wuhan Science and Technology Bureau
- Wuhan Knowledge Innovation Project
Zitieren
APA
Xiong, Y., Jiang, R., Li, Y., & Li, P. (2025). Residual Flexural Behavior of Hybrid Fiber-Reinforced Geopolymer After High Temperature Exposure. Materials, 18(15), 3572. https://doi.org/10.3390/ma18153572
Vancouver
Xiong Y, Jiang R, Li Y, Li P. Residual Flexural Behavior of Hybrid Fiber-Reinforced Geopolymer After High Temperature Exposure. Materials. 2025;18(15):3572. doi:10.3390/ma18153572
BibTeX
@article{Xiong2025,
author = {Xiong, Yiyang and Jiang, Ruiwen and Li, Yi and Li, Peipeng},
title = {Residual Flexural Behavior of Hybrid Fiber-Reinforced Geopolymer After High Temperature Exposure},
journal = {Materials},
year = {2025},
volume = {18},
number = {15},
pages = {3572},
doi = {10.3390/ma18153572}
}
EUVIMED