Improving Laser Powder Bed Fusion IN718 Process Development Efficiency by Eliminating Pore Defects of Specified Size
Materials · 24.04.2025 · 18 (9) · 1929
DOI: 10.3390/ma18091929 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 24.04.2025. Verfasst von Yuzhong Wang und 10 weiteren Autor:innen. Beteiligte Einrichtung: School of Mechanical Engineering, Xi'an Jiaotong University, Xi'an 710049, China. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the Ministry of Science and Technology of the People's Republic of China, Shaanxi Provincial Science and Technology Department common technology research and development project, Shaanxi Provincial Science and Technology Department key research and development program.
Abstract (Originalsprache)
The rapid identification of process windows in laser powder bed fusion (L-PBF) additive manufacturing garnered significant attention for its ability to reduce upfront engineering costs. This study focuses on accelerating the development of process windows by targeting the elimination of specific-size pore defects in L-PBF IN718. A novel relative density–porosity similarity evaluation method (DPSEM) is introduced to evaluate the reliability of porosity data derived from computed tomography (CT). Using the response surface method, the fully dense forming window (e.g., relative density ≥ 99%) was accurately located within a wide process parameter range (18–1000 J/mm3) in a single test. Comparative analysis with the relative density (RD) model highlighted differences in solution set distribution, positioning efficiency, microstructure, and performance within the process window. Results demonstrate that the proposed method effectively eliminates specified size defects (90 μm), achieving a maximum density of 99.5% alongside excellent mechanical properties, including an ultimate tensile strength of 1155 MPa and a yield strength of 908 MPa. In contrast, the RD model achieved a lower maximum density of 98.5%, with mechanical performance compromised by significant MC compound precipitation and keyhole pore accumulation, resulting in an ultimate tensile strength slightly exceeding 910 MPa.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- School of Mechanical Engineering, Xi'an Jiaotong University, Xi'an 710049, China.
- National Innovation Institute of Additive Manufacturing, Xi'an 710300, China.
- State Key Laboratory for Manufacturing System Engineering, Xi'an 710054, China.
ORCID-Profile: Rui Han, Chenwei Wang
Förderung
- the Ministry of Science and Technology of the People's Republic of China
- Shaanxi Provincial Science and Technology Department common technology research and development project
- Shaanxi Provincial Science and Technology Department key research and development program
- the Ministry of Science and Technology of the People’s Republic of China
- Science and Technology Department of Shaanxi Province
Zitieren
APA
Wang, Y., Guo, W., Li, W., Zhang, Y., Ma, K., Ji, Q., Han, R., Zhang, Y., Wang, C., Zhao, S., & Lu, B. (2025). Improving Laser Powder Bed Fusion IN718 Process Development Efficiency by Eliminating Pore Defects of Specified Size. Materials, 18(9), 1929. https://doi.org/10.3390/ma18091929
Vancouver
Wang Y, Guo W, Li W, Zhang Y, Ma K, Ji Q, et al. Improving Laser Powder Bed Fusion IN718 Process Development Efficiency by Eliminating Pore Defects of Specified Size. Materials. 2025;18(9):1929. doi:10.3390/ma18091929
BibTeX
@article{Wang2025,
author = {Wang, Yuzhong and Guo, Wenhua and Li, Wenxian and Zhang, Yaru and Ma, Kaiyue and Ji, Qianyu and Han, Rui and Zhang, Yihui and Wang, Chenwei and Zhao, Sihang and Lu, Bingheng},
title = {Improving Laser Powder Bed Fusion IN718 Process Development Efficiency by Eliminating Pore Defects of Specified Size},
journal = {Materials},
year = {2025},
volume = {18},
number = {9},
pages = {1929},
doi = {10.3390/ma18091929}
}
EUVIMED