Study on Molten Pool Flow and Porosity Defects in Laser–Tungsten Inert Gas (TIG) Welding of 4J36 Invar Steel
Materials · 16.04.2025 · 18 (8) · 1824
DOI: 10.3390/ma18081824 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 16.04.2025. Verfasst von Sen Wu und 4 weiteren Autor:innen. Beteiligte Einrichtung: College of Material Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, National Key Research and Development Program of China, Fundamental Research Program of Shanxi Province.
Abstract (Originalsprache)
The Invar steel molten pool is characterized by low fluidity of the molten pool due to high tension, which hinders the escape of gases and exacerbates the formation of porosity defects. In this study, the influences of different welding process parameters, material properties, and U-groove on the flow behavior of the molten pool of laser–tungsten inert gas (TIG) hybrid welding of Invar steel are investigated by numerical simulation and high-speed photography. This research proposes effective measures to suppress porosity defects, such as optimizing process parameters and extending the existence time of the molten pool. In conclusion, this study systematically investigates the dynamic mechanism of the formation of welding defects in 4J36 Invar steel and provides important theoretical support for the optimization of the welding process of 4J36 Invar steel. The results indicate that controlling the laser power at 4–6 kW, welding speed at 0.5–1.0 m/min, and welding current at 150–170 A can stabilize the molten pool flow and keyhole and promote the molten pool flow and gas escape.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- College of Material Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China.
- Shanxi Innovation Center of Metal Joining and Additive Manufacturing Technology, Taiyuan 030024, China.
- Aviation Manufacturing Technology Research Institute of China, Beijing 100024, China.
ORCID-Profile: Fei Zhao
Förderung
- National Natural Science Foundation of China
- National Key Research and Development Program of China
- Fundamental Research Program of Shanxi Province
Zitieren
APA
Wu, S., Zhao, F., Wang, P., Gong, S., & Wu, Z. (2025). Study on Molten Pool Flow and Porosity Defects in Laser–Tungsten Inert Gas (TIG) Welding of 4J36 Invar Steel. Materials, 18(8), 1824. https://doi.org/10.3390/ma18081824
Vancouver
Wu S, Zhao F, Wang P, Gong S, Wu Z. Study on Molten Pool Flow and Porosity Defects in Laser–Tungsten Inert Gas (TIG) Welding of 4J36 Invar Steel. Materials. 2025;18(8):1824. doi:10.3390/ma18081824
BibTeX
@article{Wu2025,
author = {Wu, Sen and Zhao, Fei and Wang, Pengfei and Gong, Shuili and Wu, Zhisheng},
title = {Study on Molten Pool Flow and Porosity Defects in Laser–Tungsten Inert Gas (TIG) Welding of 4J36 Invar Steel},
journal = {Materials},
year = {2025},
volume = {18},
number = {8},
pages = {1824},
doi = {10.3390/ma18081824}
}
EUVIMED