EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Diamond Wire Wear and Its Effect on Surface Quality in Cutting of Monocrystalline Silicon

Jinguang Du, Yu Wu, Zhen Zhang iD, Yu Zhang, Wenbin He, Junxiao Geng, Liuyang Duan, Wuyi Ming

Materials · 12.04.2025 · 18 (8) · 1768

DOI: 10.3390/ma18081768 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 12.04.2025. Verfasst von Jinguang Du und 7 weiteren Autor:innen. Beteiligte Einrichtung: Henan Provincial Key Laboratory of Intelligent Manufacturing of Mechanical Equipment, Zhengzhou University of Light Industry, Zhengzhou 450002, China. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Guangdong HUST Industrial Technology Research Institute, Guangdong Provincial Key Laboratory of Manufacturing Equipment Digitization, Key Research and Development Projects of Henan Province.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Monocrystalline silicon is widely used in the semiconductor industry. During wafer machining with a diamond wire saw (DWS), a worn diamond wire can affect the slicing quality. To assess the effect of diamond wire wear on wafer machining, in this study, the impact of diamond wire wear on the wafer’s total thickness variation (TTV) and surface quality was examined at a wire velocity of 1.8 m/s and a feed rate of 0.5 mm/min. Through a single-factor experiment, the effects of the wire velocity, feed rate, and workpiece thickness on diamond wire wear were explored. The outcomes demonstrate that the wear rate was higher in the early and late wear periods, and the wafer machining quality was poor in these two periods. During the stable wear period, the machined wafer exhibited high quality, while the wear rate remained stable. Under the condition of machining the same area of the workpiece, with an increase in wire velocity, the wear quantity for the diamond wire was reduced. As the feed rate and workpiece thickness increased, the wear quantity of the diamond wire increased. The diamond wire wear remained roughly constant when the wire velocity and feed rate increased at the same ratio.

Schlagwörter

Stichwörter der Autor:innen

abrasive weardiamond wire saw (DWS)monocrystalline siliconsurface roughnesstotal thickness variation (TTV)

Autor:innen und Institutionen

  • Henan Provincial Key Laboratory of Intelligent Manufacturing of Mechanical Equipment, Zhengzhou University of Light Industry, Zhengzhou 450002, China.
  • Henan Province Engineering Technology Research Center of Green Manufacturing and Precision Measurement, Zhengzhou University of Light Industry, Zhengzhou 450002, China.
  • School of Aerospace Engineering, Huazhong University of Science and Technology, Wuhan 430074, China.
  • Guangdong Provincial Key Laboratory of Digital Manufacturing Equipment, Guangdong HUST Industrial Technology Research Institute, Dongguan 523808, China.

ORCID-Profile: Zhen Zhang

Förderung

  • Guangdong HUST Industrial Technology Research Institute, Guangdong Provincial Key Laboratory of Manufacturing Equipment Digitization
  • Key Research and Development Projects of Henan Province

Zitieren

APA

Du, J., Wu, Y., Zhang, Z., Zhang, Y., He, W., Geng, J., Duan, L., & Ming, W. (2025). Diamond Wire Wear and Its Effect on Surface Quality in Cutting of Monocrystalline Silicon. Materials, 18(8), 1768. https://doi.org/10.3390/ma18081768

Vancouver

Du J, Wu Y, Zhang Z, Zhang Y, He W, Geng J, et al. Diamond Wire Wear and Its Effect on Surface Quality in Cutting of Monocrystalline Silicon. Materials. 2025;18(8):1768. doi:10.3390/ma18081768

BibTeX
@article{Du2025,
  author = {Du, Jinguang and Wu, Yu and Zhang, Zhen and Zhang, Yu and He, Wenbin and Geng, Junxiao and Duan, Liuyang and Ming, Wuyi},
  title = {Diamond Wire Wear and Its Effect on Surface Quality in Cutting of Monocrystalline Silicon},
  journal = {Materials},
  year = {2025},
  volume = {18},
  number = {8},
  pages = {1768},
  doi = {10.3390/ma18081768}
}
Kostenlos starten →