Fracture Toughness of Short Fibre-Reinforced Composites—In Vitro Study
Materials · 02.11.2024 · 17 (21) · 5368
DOI: 10.3390/ma17215368 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 02.11.2024. Verfasst von Noor Kamourieh und 4 weiteren Autor:innen. Beteiligte Einrichtung: UCL Eastman Dental Institute, London WC1E 6DE, UK. Die Arbeit wurde bisher 14-mal zitiert (Crossref) und nennt 46 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).
Abstract (Originalsprache)
The development of dental materials needs to be supported with sound evidence. This in vitro study aimed to measure the fracture toughness of a short fibre-reinforced composite (sFRC), at differing thicknesses. In this study, 2 mm, 3 mm and 4 mm depths of sFRC were prepared. Using ISO4049, each preparation was tested to failure. A total of 60 samples were tested: 10 samples for each combination of sFRC and depth. Fractured samples were viewed, and outcomes were analysed. EXF showed greater toughness than EXP, with a mean of 2.49 (95%CI: 2.25, 2.73) MPa.m1/2 compared to a mean of 2.13 (95%CI: 1.95, 2.31) MPa.m1/2, (F(1,54) = 21.28; p < 0.001). This difference was particularly pronounced at 2 mm depths where the mean (95%CI) values were 2.72 (2.49, 2.95) for EXF and 1.90 (1.78, 2.02) for EXP (Interaction F(2,54) = 7.93; p < 0.001). Both materials performed similarly at the depths of 3 mm and 4 mm. The results for both materials were within the accepted fracture toughness values of dentine of 1.79–3.08 MPa.m1/2. Analysis showed crack deflection and bridging fibre behaviour. The optimal thickness at the cavity base for EXF was 2 mm and for EXP 4 mm. Crack deflection and bridging behaviour indicated that restorations incorporating sFRCs are not prone to catastrophic failure and confirmed that sFRCs have similar fracture toughness to dentine. sFRCs could be a suitable biomimetic material to replace dentine.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- UCL Eastman Dental Institute, London WC1E 6DE, UK.
ORCID-Profile: Albert Leung, Peter Fine
Zitieren
APA
Kamourieh, N., Faigenblum, M., Blizard, R., Leung, A., & Fine, P. (2024). Fracture Toughness of Short Fibre-Reinforced Composites—In Vitro Study. Materials, 17(21), 5368. https://doi.org/10.3390/ma17215368
Vancouver
Kamourieh N, Faigenblum M, Blizard R, Leung A, Fine P. Fracture Toughness of Short Fibre-Reinforced Composites—In Vitro Study. Materials. 2024;17(21):5368. doi:10.3390/ma17215368
BibTeX
@article{Kamourieh2024,
author = {Kamourieh, Noor and Faigenblum, Maurice and Blizard, Robert and Leung, Albert and Fine, Peter},
title = {Fracture Toughness of Short Fibre-Reinforced Composites—In Vitro Study},
journal = {Materials},
year = {2024},
volume = {17},
number = {21},
pages = {5368},
doi = {10.3390/ma17215368}
}
EUVIMED