EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Welding Characteristics of Medium Titanium Plates with Autogenous Laser Welding and Narrow-Gap Laser Filling Welding Modes

Junzhao Li, Hang Yu, Xin Yin, Bin Kong, Kai Wen, Qingjie Sun, Bingfeng Wang iD, Xianshan Zeng

Materials · 26.09.2024 · 17 (19) · 4722

DOI: 10.3390/ma17194722 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 26.09.2024. Verfasst von Junzhao Li und 7 weiteren Autor:innen. Beteiligte Einrichtung: School of Materials Science and Engineering, Central South University, Changsha 410083, China. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 23 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: The science and technology innovation program of Hunan province, science and technology innovation program of Hunan province.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Titanium and titanium alloys with a medium thickness of 5 to 12 mm are widely used for ocean platforms, military equipment and in other fields because of their light weight, appropriate strength and corrosion resistance. In this study, autogenous laser welding and narrow-gap laser welding processes were researched and compared, and the welding characteristics, weld microstructure and joint strength were analyzed. The results showed that autogenous laser welding had higher efficiency, narrower weld width and higher microstructure uniformity. Autogenous laser welding can achieve the single pass weld penetration at laser keyhole mode. The weld width of narrow-gap laser welded joint was 12.5 mm, which was nearly three times than that of autogenous laser welding. The grain size of autogenous laser welding was obviously smaller and more uniform in depth than that of narrow-gap laser welding. In the weld zone, the coarse columnar α grains grew from the fusion line, while in the heat-affected zone, equiaxed α grains with needle and sawtooth α morphologies were presented. The microhardness of the heat-affected zone was higher than in the weld zone and the base metal due to the denser needle microstructure. The tensile samples all fractured at the base metal, indicating the welded joint strength efficiency was greater than 1.

Schlagwörter

Stichwörter der Autor:innen

autogenous laser weldingmedium platenarrow-gap laser weldingpure titanium

Autor:innen und Institutionen

  • School of Materials Science and Engineering, Central South University, Changsha 410083, China.
  • Hunan Xiangtou Goldsky Titanium Metal Co., Ltd., Changsha 410083, China.
  • Hunan Xiangtou Goldsky New Materials Co., Ltd., Yiyang 413000, China.
  • Shandong Provincial Key Laboratory of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264209, China.

ORCID-Profile: Bingfeng Wang

Förderung

  • The science and technology innovation program of Hunan province
  • science and technology innovation program of Hunan province

Zitieren

APA

Li, J., Yu, H., Yin, X., Kong, B., Wen, K., Sun, Q., Wang, B., & Zeng, X. (2024). Welding Characteristics of Medium Titanium Plates with Autogenous Laser Welding and Narrow-Gap Laser Filling Welding Modes. Materials, 17(19), 4722. https://doi.org/10.3390/ma17194722

Vancouver

Li J, Yu H, Yin X, Kong B, Wen K, Sun Q, et al. Welding Characteristics of Medium Titanium Plates with Autogenous Laser Welding and Narrow-Gap Laser Filling Welding Modes. Materials. 2024;17(19):4722. doi:10.3390/ma17194722

BibTeX
@article{Li2024,
  author = {Li, Junzhao and Yu, Hang and Yin, Xin and Kong, Bin and Wen, Kai and Sun, Qingjie and Wang, Bingfeng and Zeng, Xianshan},
  title = {Welding Characteristics of Medium Titanium Plates with Autogenous Laser Welding and Narrow-Gap Laser Filling Welding Modes},
  journal = {Materials},
  year = {2024},
  volume = {17},
  number = {19},
  pages = {4722},
  doi = {10.3390/ma17194722}
}
Kostenlos starten →