Fachartikel in der Zeitschrift Materials, online erschienen am 10.09.2024. Verfasst von Yali Gao und 6 weiteren Autor:innen. Beteiligte Einrichtung: Department of Mechanical Engineering, Northeast Electric Power University, No. 169 Changchun Road, Jilin 132012, China. Die Arbeit wurde bisher 10-mal zitiert (Crossref) und nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the Project of Science and Technology research of Department of Education of Jilin Province, the Natural Science Foundation of Science and Technology Department of Jilin Province.
Abstract (Originalsprache)
In order to prepare coating with good friction and wear resistance at elevated temperature on the surface of hot-working tool steel, by using a CO2 laser, FeCrNiTiZr high-entropy alloy coating with different laser scanning speeds (360, 480 and 600 mm/min, respectively) was successfully fabricated by using laser cladding technology on the surface of H13 steel in this paper. Phase constitutions, microhardness, microstructure, and wear characteristics of FeCrNiTiZr coatings under different laser scanning speeds were analyzed. It was determined that 480 mm/min was the optimal laser scanning speed. The results showed that the coating at the scanning speed of 480 mm/min consists of a BCC phase with significant lattice distortion and high dislocation density; the crystal structure is cellular crystal and dendrite crystal. The coating demonstrates the highest microhardness (842 HV0.2), which is 4.2 times that of the substrate (200 HV0.2). Its average friction coefficients at room temperature and 823 K are approximately one-seventh and one-third of the substrate’s, respectively, and its wear volume is reduced by about 98% and 81% under these conditions. Compared to the substrate, the coating underwent slight abrasive wear, adhesive wear, and oxidative wear at both room temperature and 823 K. In contrast, the substrate underwent severe abrasive wear, adhesive wear, oxidative wear, and even fatigue wear.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Mechanical Engineering, Northeast Electric Power University, No. 169 Changchun Road, Jilin 132012, China.
- School of Mechanical Electrical Engineering, Jilin Institute of Chemical Technology, Jilin 132022, China.
ORCID-Profile: Yali Gao
Förderung
- the Project of Science and Technology research of Department of Education of Jilin Province
- the Natural Science Foundation of Science and Technology Department of Jilin Province
Zitieren
APA
Gao, Y., Bai, S., Jiang, S., Lu, P., Zhang, D., Jie, M., & Liu, Y. (2024). Effect of the Laser Cladding Parameters on Microstructure and Elevated Temperature Wear of FeCrNiTiZr Coatings. Materials, 17(18), 4444. https://doi.org/10.3390/ma17184444
Vancouver
Gao Y, Bai S, Jiang S, Lu P, Zhang D, Jie M, et al. Effect of the Laser Cladding Parameters on Microstructure and Elevated Temperature Wear of FeCrNiTiZr Coatings. Materials. 2024;17(18):4444. doi:10.3390/ma17184444
BibTeX
@article{Gao2024,
author = {Gao, Yali and Bai, Sicheng and Jiang, Shan and Lu, Pengyong and Zhang, Dongdong and Jie, Meng and Liu, Yu},
title = {Effect of the Laser Cladding Parameters on Microstructure and Elevated Temperature Wear of FeCrNiTiZr Coatings},
journal = {Materials},
year = {2024},
volume = {17},
number = {18},
pages = {4444},
doi = {10.3390/ma17184444}
}
EUVIMED