In Situ Fabrication of TiC/Ti–Matrix Composites by Laser Directed Energy Deposition
Materials · 29.08.2024 · 17 (17) · 4284
DOI: 10.3390/ma17174284 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials, online erschienen am 29.08.2024. Verfasst von Sabin Mihai und 4 weiteren Autor:innen. Beteiligte Einrichtung: Center for Advanced Laser Technologies (CETAL), National Institute for Laser, Plasma and Radiation Physics (INFLPR), 077125 Magurele, Romania. Die Arbeit wurde bisher 25-mal zitiert (Crossref) und nennt 51 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Unitatea Executiva Pentru Finantarea Invatamantului Superior a Cercetarii Dezvoltarii si Inovarii, Romanian Ministry of Research, Innovation and Digitalization under Romanian National Core Program LAPLAS VII, Romanian Ministry of Education and Research.
Abstract (Originalsprache)
In this study, crack-free TiC/Ti composites with TiC content ranging from 0 to 15 wt.% were successfully fabricated using Direct Energy Deposition with a dual-feeder system that concomitantly delivered different amounts of both constituents into a high-power laser beam. The samples were investigated to evaluate the morphologies and distribution behavior of TiC. The microhardness values of the samples obtained under optimal processing conditions increased from 192 ± 5.3 HV0.2 (pure Ti) to 300 ± 14.2 HV0.2 (Ti + wt.% 15 TiC). Also, TiC has a significant impact on the Ti matrix, increasing the strength of TMCs up to 725 ± 5.4 MPa, while the elongation drastically decreased to 0.62 ± 0.04%. The wear rate is not proportionally affected by the rise content of TiC reinforcement; the hypoeutectic region of TMCs exhibited a wear rate of 2.45 mm3/N·m (Ti + wt.% 3 TiC) and a friction coefficient of 0.48 compared to the ones from the hypereutectic region, which measured a wear rate of 3.02 mm3/N·m (Ti + wt.% 15 TiC) and a friction coefficient of 0.63. The improved values of mechanical properties in the case of TMCs as compared to pure Ti are provided due to the solid solution strengthening of carbon and the fine grain strengthening. This work outlines a method for changing TiC morphologies to improve the hardness and tensile strength of TMCs fabricated starting from micro-scale powder.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Center for Advanced Laser Technologies (CETAL), National Institute for Laser, Plasma and Radiation Physics (INFLPR), 077125 Magurele, Romania.
- Faculty of Industrial Engineering and Robotics, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania.
- Faculty of Applied Sciences, National University of Science and Technology Politehnica Bucharest, 060042 Bucharest, Romania.
ORCID-Profile: Florin Baciu
Förderung
- Unitatea Executiva Pentru Finantarea Invatamantului Superior a Cercetarii Dezvoltarii si Inovarii
- Romanian Ministry of Research, Innovation and Digitalization under Romanian National Core Program LAPLAS VII
- Romanian Ministry of Education and Research
Zitieren
APA
Mihai, S., Baciu, F., Radu, R., Chioibasu, D., & Popescu, A. C. (2024). In Situ Fabrication of TiC/Ti–Matrix Composites by Laser Directed Energy Deposition. Materials, 17(17), 4284. https://doi.org/10.3390/ma17174284
Vancouver
Mihai S, Baciu F, Radu R, Chioibasu D, Popescu AC. In Situ Fabrication of TiC/Ti–Matrix Composites by Laser Directed Energy Deposition. Materials. 2024;17(17):4284. doi:10.3390/ma17174284
BibTeX
@article{Mihai2024,
author = {Mihai, Sabin and Baciu, Florin and Radu, Robert and Chioibasu, Diana and Popescu, Andrei C},
title = {In Situ Fabrication of TiC/Ti–Matrix Composites by Laser Directed Energy Deposition},
journal = {Materials},
year = {2024},
volume = {17},
number = {17},
pages = {4284},
doi = {10.3390/ma17174284}
}
EUVIMED