Fachartikel in der Zeitschrift Materials, online erschienen am 22.07.2024. Verfasst von Kai Li und 3 weiteren Autor:innen. Beteiligte Einrichtung: Guiyang Water Environment Group Co., Ltd., Guiyang 550025, China. Die Arbeit wurde bisher 24-mal zitiert (Crossref) und nennt 77 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Zhonghu Wu, Guizhou Science and Technology Fund.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Phosphogypsum (PG) occupies a large amount of land due to its large annual production and low utilization rate, and at the same time causes serious environmental problems due to toxic impurities. PG is used for mine backfill, and industrial solid waste is a curing agent for PG, which can save the filling cost and reduce environmental pollution. In this paper, PG was used as a raw material, combined with steel slag (SS) and ground granulated blast-furnace slag (GGBS) under the action of an alkali-activated agent (NaOH) to prepare all-solid waste phosphogypsum-based backfill material (PBM). The effect of the GGBS to SS ratio on the compressive strength and toxic leaching of PBM was investigated. The chemical composition of the raw materials was obtained by XRF analysis, and the mineral composition and morphology of PBM and its stabilization/curing mechanism against heavy metals were analyzed using XRD and SEM-EDS. The results showed that the best performance of PBM was achieved when the contents of PG, GGBS, and SS were 80%, 13%, and 7%, the liquid-to-solid ratio was 0.4, and the mass concentration of NaOH was 4%, with a strength of 2.8 MPa at 28 days. The leaching concentration of fluorine at 7 days met the standard of groundwater class IV (2 mg/L), and the leaching concentration of phosphorus was detected to be less than 0.001 mg/L, and the leaching concentration of heavy metals met the environmental standard at 14 d. The hydration concentration in PBM met the environmental standard. The hydration products in PBM are mainly ettringite and C-(A)-S-H gel, which can effectively stabilize the heavy metals in PG through chemical precipitation, physical adsorption, and encapsulation.

Schlagwörter

Stichwörter der Autor:innen

all-solid waste backfill materialsground granulated blast-furnace slagmicromechanismsphosphogypsumsteel slagtoxic leaching

Autor:innen und Institutionen

  • Guiyang Water Environment Group Co., Ltd., Guiyang 550025, China.
  • College of Civil Engineering, Guizhou University, Guiyang 550025, China.

Förderung

  • Zhonghu Wu
  • Guizhou Science and Technology Fund

Zitieren

APA

Li, K., Zhu, L., Wu, Z., & Wang, X. (2024). Properties of Cemented Filling Materials Prepared from Phosphogypsum-Steel Slag–Blast-Furnace Slag and Its Environmental Effect. Materials, 17(14), 3618. https://doi.org/10.3390/ma17143618

Vancouver

Li K, Zhu L, Wu Z, Wang X. Properties of Cemented Filling Materials Prepared from Phosphogypsum-Steel Slag–Blast-Furnace Slag and Its Environmental Effect. Materials. 2024;17(14):3618. doi:10.3390/ma17143618

BibTeX
@article{Li2024,
  author = {Li, Kai and Zhu, Lishun and Wu, Zhonghu and Wang, Xiaomin},
  title = {Properties of Cemented Filling Materials Prepared from Phosphogypsum-Steel Slag–Blast-Furnace Slag and Its Environmental Effect},
  journal = {Materials},
  year = {2024},
  volume = {17},
  number = {14},
  pages = {3618},
  doi = {10.3390/ma17143618}
}
Kostenlos starten →