Fachartikel in der Zeitschrift Materials, online erschienen am 09.05.2024. Verfasst von Shiyu Wang und 3 weiteren Autor:innen. Beteiligte Einrichtung: College of Materials Science and Engineering, Xi'an University of Architecture & Technology, Xi'an 710055, China. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: "the 14th Five-Year" National Science and Technology Major Project of China, Shaanxi Provincial Innovation Capability Support Program, “the 14th Five-Year” National Science and Technology Major Project of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The production of flue gas desulfurization gypsum poses a serious threat to the environment. Thus, utilizing gypsum-based self-leveling mortar (GSLM) stands out as a promising and effective approach to address the issue. β-hemihydrate gypsum, cement, polycarboxylate superplasticizer, hydroxypropyl methyl cellulose ether (HPMC), retarder, and defoamer were used to prepare GSLM. The impact of mineral admixtures (steel slag (SS), silica fume (SF), and fly ash (FA)) on the physical, mechanical, and microstructural properties of GSLM was examined through hydration heat, X-ray diffractometry (XRD), Raman spectroscopy, and scanning electron microscopy (SEM) analyses. The GSLM benchmark mix ratio was determined as follows: 94% of desulfurization building gypsum, 6% of cement, 0.638% each of water reducer and retarder, 0.085% each of HPMC and defoamer (calculated additive ratio relative to gypsum), and 0.54 water-to-cement ratio. Although the initial fluidity decreased in the GSLM slurry with silica fume, there was minimal change in 30 min fluidity. Notably, at an SS content of 16%, the GSLM exhibited optimal flexural strength (6.6 MPa) and compressive strength (20.4 MPa). Hydration heat, XRD, and Raman analyses revealed that a small portion of SS actively participated in the hydration reaction, while the remaining SS served as a filler.

Schlagwörter

Stichwörter der Autor:innen

flue gas desulfurization gypsum-based self-leveling mortarfly ashpropertiessilica fumesteel slag

Autor:innen und Institutionen

  • College of Materials Science and Engineering, Xi'an University of Architecture & Technology, Xi'an 710055, China.

ORCID-Profile: Chang Chen

Förderung

  • "the 14th Five-Year" National Science and Technology Major Project of China
  • Shaanxi Provincial Innovation Capability Support Program
  • “the 14th Five-Year” National Science and Technology Major Project of China

Zitieren

APA

Wang, S., Chen, Y., Zhao, W., & Chen, C. (2024). Effect of Mineral Admixtures on Physical, Mechanical, and Microstructural Properties of Flue Gas Desulfurization Gypsum-Based Self-Leveling Mortar. Materials, 17(10), 2227. https://doi.org/10.3390/ma17102227

Vancouver

Wang S, Chen Y, Zhao W, Chen C. Effect of Mineral Admixtures on Physical, Mechanical, and Microstructural Properties of Flue Gas Desulfurization Gypsum-Based Self-Leveling Mortar. Materials. 2024;17(10):2227. doi:10.3390/ma17102227

BibTeX
@article{Wang2024,
  author = {Wang, Shiyu and Chen, Yanxin and Zhao, Wei and Chen, Chang},
  title = {Effect of Mineral Admixtures on Physical, Mechanical, and Microstructural Properties of Flue Gas Desulfurization Gypsum-Based Self-Leveling Mortar},
  journal = {Materials},
  year = {2024},
  volume = {17},
  number = {10},
  pages = {2227},
  doi = {10.3390/ma17102227}
}
Kostenlos starten →