Shear Bond Strength between Orthodontic Brackets and Monolithic 4Y-TZP: An In Vitro Study

Emre Cakir, Ayse Nurcan Duman, Arzu Zeynep Yildirim, Pinar Cevik iD

Materials · 23.07.2023 · 16 (14) · 5173

DOI: 10.3390/ma16145173 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 23.07.2023. Verfasst von Emre Cakir und 3 weiteren Autor:innen. Beteiligte Einrichtung: Private Practice, Ankara 06420, Türkiye. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 44 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The aim of this study was to evaluate the effect of different surface treatments on the shear bond strength (SBS) between metal orthodontic brackets and monolithic zirconia surfaces bonded with resin composite. Fifty monolithic zirconia (4Y-TZP) disks were sintered and glazed. Specimens were divided into five groups (n = 10) for different surface treatments: control, nano second fiber laser, sandblasting, grinding and tribochemical coating (CoJet Sand 30-μm). Metal orthodontic brackets were bonded to monolithic zirconia surface by two-component orthodontic adhesive. After 500 cycles of thermocycling, shear bond strength values were measured by a universal testing machine at a cross head speed of 0.5 mm/min. The data was recorded as MPa and statistically analyzed with One-way ANOVA, Levene’s LSD tests with Bonferroni corrections. The significance level was α = 0.05. The surface topography of one specimen of each group was evaluated by scanning electron microscopy (SEM). Statistically significant difference was observed among study groups (p = 0.018). The lowest shear bond strength was observed in the control group (3.92 ± 1.9). Tribochemical coating showed the highest bond strength (7.44 ± 2.9), which was statistically different from the control and nano second laser (4.3 ± 1.4) groups but not statistically different from grinding (6.15 ± 3.1) or sandblasting (6.47 ± 3.3). SEM images showed comprehensive results of each surface treatment on monolithic zirconia. All failure modes were recorded as adhesive between the composite resin and monolithic zirconia. Based on the findings of this study, it can be concluded that grinding, sandblasting and tribochemical coating techniques showed clinically acceptable bond strength within the range of 6–8 MPa. These surface treatments can be considered suitable for achieving a durable bond between metal orthodontic brackets and monolithic 4Y-TZP ceramic surfaces.

Schlagwörter

Stichwörter der Autor:innen

bondinglasersorthodontic bracketresin compositeshear strengthyttria stabilized tetragonal zirconia

Autor:innen und Institutionen

  • Private Practice, Ankara 06420, Türkiye.
  • Department of Prosthodontics, Faculty of Dentistry, Gazi University, Ankara 06490, Türkiye.
  • Department of General Practice and Dental Public Health, School of Dentistry, The University of Texas Health Science Center at Houston, Houston, TX 77054, USA.
  • Houston Center for Biomaterials and Biomimetics, Houston, TX 77054, USA.

ORCID-Profile: Pinar Cevik

Zitieren

APA

Cakir, E., Duman, A. N., Yildirim, A. Z., & Cevik, P. (2023). Shear Bond Strength between Orthodontic Brackets and Monolithic 4Y-TZP: An In Vitro Study. Materials, 16(14), 5173. https://doi.org/10.3390/ma16145173

Vancouver

Cakir E, Duman AN, Yildirim AZ, Cevik P. Shear Bond Strength between Orthodontic Brackets and Monolithic 4Y-TZP: An In Vitro Study. Materials. 2023;16(14):5173. doi:10.3390/ma16145173

BibTeX
@article{Cakir2023,
  author = {Cakir, Emre and Duman, Ayse Nurcan and Yildirim, Arzu Zeynep and Cevik, Pinar},
  title = {Shear Bond Strength between Orthodontic Brackets and Monolithic 4Y-TZP: An In Vitro Study},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {14},
  pages = {5173},
  doi = {10.3390/ma16145173}
}
Kostenlos starten →