Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 18.06.2023. Verfasst von Ziyue Zhao und 5 weiteren Autor:innen. Beteiligte Einrichtung: Center for Advanced Low-Dimension Materials, State Key Laboratory for Modification of Chemical Fibers and Polymer Materials, College of Materials Sci…. Die Arbeit wurde bisher 25-mal zitiert (Crossref) und nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key R&D Program of China, National Key R&D Program of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This paper used poly (aryl ether ketone) (PAEK) resin with a low melting temperature to prepare laminate via the compression-molding process for continuous-carbon-fiber-reinforced composites (CCF-PAEK). Then, poly (ether ether ketone) (PEEK), or a short-carbon-fiber-reinforced poly (ether ether ketone) (SCF-PEEK) with a high melting temperature, was injected to prepare the overmolding composites. The shear strength of short beams was used to characterize the interface bonding strength of composites. The results showed that the interface properties of the composite were affected by the interface temperature, which was adjusted by mold temperature. PAEK and PEEK formed a better interfacial bonding at higher interface temperatures. The shear strength of the SCF-PEEK/CCF-PAEK short beam was 77 MPa when the mold temperature was 220 °C and 85 MPa when the mold temperature was raised to 260 °C. The melting temperature did not significantly affect the shear strength of SCF-PEEK/CCF-PAEK short beams. For the melting temperature increasing from 380 °C to 420 °C, the shear strength of the SCF-PEEK/CCF-PAEK short beam ranged from 83 MPa to 87 MPa. The microstructure and failure morphology of the composite was observed using an optical microscope. A molecular dynamics model was established to simulate the adhesion of PAEK and PEEK at different mold temperatures. The interfacial bonding energy and diffusion coefficient agreed with the experimental results.

Schlagwörter

Stichwörter der Autor:innen

interfacial propertiesmolecular dynamics simulationovermoldingpoly (aryl ether ketone)poly (ether ether ketone)

Autor:innen und Institutionen

  • Center for Advanced Low-Dimension Materials, State Key Laboratory for Modification of Chemical Fibers and Polymer Materials, College of Materials Science and Engineering, Donghua University, Shanghai 201620, China.

ORCID-Profile: Jindong Zhang

Förderung

  • National Key R&D Program of China
  • National Key R&D Program of China

Zitieren

APA

Zhao, Z., Zhang, J., Bi, R., Chen, C., Yao, J., & Liu, G. (2023). Study on the Overmolding Process of Carbon-Fiber-Reinforced Poly (Aryl Ether Ketone) (PAEK)/Poly (Ether Ether Ketone) (PEEK) Thermoplastic Composites. Materials, 16(12), 4456. https://doi.org/10.3390/ma16124456

Vancouver

Zhao Z, Zhang J, Bi R, Chen C, Yao J, Liu G. Study on the Overmolding Process of Carbon-Fiber-Reinforced Poly (Aryl Ether Ketone) (PAEK)/Poly (Ether Ether Ketone) (PEEK) Thermoplastic Composites. Materials. 2023;16(12):4456. doi:10.3390/ma16124456

BibTeX
@article{Zhao2023,
  author = {Zhao, Ziyue and Zhang, Jindong and Bi, Ran and Chen, Chunhai and Yao, Jianan and Liu, Gang},
  title = {Study on the Overmolding Process of Carbon-Fiber-Reinforced Poly (Aryl Ether Ketone) (PAEK)/Poly (Ether Ether Ketone) (PEEK) Thermoplastic Composites},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {12},
  pages = {4456},
  doi = {10.3390/ma16124456}
}
Kostenlos starten →