EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Microstructure Evolution with Rapid Thermal Annealing Time in (001)-Oriented Piezoelectric PZT Films Integrated on (111) Si

Yingying Wang, Hanfei Zhu, Yinxiu Xue, Peng Yan, Jun Ouyang iD

Materials · 02.03.2023 · 16 (5) · 2068

DOI: 10.3390/ma16052068 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 02.03.2023. Verfasst von Yingying Wang und 4 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory for Liquid-Solid Structure Evolution and Processing of Materials (Ministry of Education), School of Materials Science and Engineering,…. Die Arbeit wurde bisher 12-mal zitiert (Crossref) und nennt 35 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Hanfei Zhu, J. Ouyang, National Natural Science Foundation of China (NSFC).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In our recently published paper (Y.-Y. Wang et al., High performance LaNiO3-buffered, (001)-oriented PZT piezoelectric films integrated on (111) Si, Appl. Phys. Lett. 121, 182902, 2022), highly (001)-oriented PZT films with a large transverse piezoelectric coefficient e31,f prepared on (111) Si substrates were reported. This work is beneficial for the development of piezoelectric micro-electro-mechanical systems (Piezo-MEMS) because of (111) Si’s isotropic mechanical properties and desirable etching characteristics. However, the underlying mechanism for the achievement of a high piezoelectric performance in these PZT films going through a rapid thermal annealing process has not been thoroughly analyzed. In this work, we present complete sets of data in microstructure (XRD, SEM and TEM) and electrical properties (ferroelectric, dielectric and piezoelectric) for these films with typical annealing times of 2, 5, 10 and 15 min. Through data analyses, we revealed competing effects in tuning the electrical properties of these PZT films, i.e., the removal of residual PbO and proliferation of nanopores with an increasing annealing time. The latter turned out to be the dominating factor for a deteriorated piezoelectric performance. Therefore, the PZT film with the shortest annealing time of 2 min showed the largest e31,f piezoelectric coefficient. Furthermore, the performance degradation occurred in the PZT film annealed for 10 min can be explained by a film morphology change, which involved not only the change in grain shape, but also the generation of a large amount of nanopores near its bottom interface.

Schlagwörter

Stichwörter der Autor:innen

Siferroelectric filmlead zirconate titanate (PZT)micro-electro-mechanical systems (MEMS)nanoporespiezoelectricrapid thermal annealing (RTA)

Autor:innen und Institutionen

  • Key Laboratory for Liquid-Solid Structure Evolution and Processing of Materials (Ministry of Education), School of Materials Science and Engineering, Shandong University, Jinan 250061, China.
  • Institute of Advanced Energy Materials and Chemistry, School of Chemistry and Chemical Engineering, Qilu University of Technology (Shandong Academy of Sciences), Jinan 250353, China.
  • Key Laboratory of High-efficiency and Clean Mechanical Manufacturing (Ministry of Education), School of Mechanical Engineering, Shandong University, Jinan 250061, China.
  • School of Materials Science and Engineering, Xiangtan University, Xiangtan 411105, China.

ORCID-Profile: Jun Ouyang

Förderung

  • Hanfei Zhu
  • J. Ouyang
  • National Natural Science Foundation of China (NSFC)
  • Natural Science Foundation of Shandong Province
  • Science, Education and Industry Integration Pilot Projects of Qilu University of Technology (Shandong Academy of Sciences)
  • Jinan City Science and Technology Bureau
  • Education Department of Hunan Province/Xiangtan University
  • Qilu University of Technology (Shandong Academy of Sciences)

Zitieren

APA

Wang, Y., Zhu, H., Xue, Y., Yan, P., & Ouyang, J. (2023). Microstructure Evolution with Rapid Thermal Annealing Time in (001)-Oriented Piezoelectric PZT Films Integrated on (111) Si. Materials, 16(5), 2068. https://doi.org/10.3390/ma16052068

Vancouver

Wang Y, Zhu H, Xue Y, Yan P, Ouyang J. Microstructure Evolution with Rapid Thermal Annealing Time in (001)-Oriented Piezoelectric PZT Films Integrated on (111) Si. Materials. 2023;16(5):2068. doi:10.3390/ma16052068

BibTeX
@article{Wang2023,
  author = {Wang, Yingying and Zhu, Hanfei and Xue, Yinxiu and Yan, Peng and Ouyang, Jun},
  title = {Microstructure Evolution with Rapid Thermal Annealing Time in (001)-Oriented Piezoelectric PZT Films Integrated on (111) Si},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {5},
  pages = {2068},
  doi = {10.3390/ma16052068}
}
Kostenlos starten →