Processing of Haynes® 282® Alloy by Direct Energy Deposition with Arc and Wire

Manuela Zinke iD, Stefan Burger, Sven Jüttner iD

Materials · 18.02.2023 · 16 (4) · 1715

DOI: 10.3390/ma16041715 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Materials, online erschienen am 18.02.2023. Verfasst von Manuela Zinke und 2 weiteren Autor:innen. Beteiligte Einrichtung: Institute of Materials and Joining Technology, Otto von Guericke University, 39106 Magdeburg, Germany. Die Arbeit wurde bisher 12-mal zitiert (Crossref) und nennt 42 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: German Association of Joint Industrial Applied Research Institutes, German Research Association on Welding and Allied Processes (DVS), AiF (German Federation of Industrial Research Associations).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Direct energy deposition with arc and wire (DED-AW) is a versatile, low-cost, and energy-efficient technology for additive manufacturing of medium- and large-sized metallic components. In this study, the effects of arc energy and shielding gas in cold metal transfer (CMT) welding of walls and blocks on cooling time, mechanical properties, and macro- and microstructure have been studied using precipitation-hardenable Ni-based superalloy Haynes® 282®. The arc energy and consequently the cooling rate were varied by changing the wire feed rate and the travel speed. As expected, increasing the arc energy leads to higher cooling times for the walls. Due to the 2D thermal conduction, the thin walls cool down much slower than multi-layer welded blocks, but this reduces the strength values only very slightly. While the walls have no sensitivity to the occurrence of unacceptable seam irregularities, the multi-layer blocks show isolated seam defects, such as hot cracks or lack of fusion. Despite shielding gas variation, the as-welded blocks show acceptable strength properties at room temperatures (RT) and impact values at RT and −196 °C. However, the use of an N-containing shielding gas results in lower elongation and notched bar impact energy. Precipitation-hardened specimens tested at 871 °C exhibit a similar strength level to transverse tensile specimens of gas metal arc welding (GMAW) welded joints on 12.7 mm thick plates with fracture in the weld metal.

Schlagwörter

Stichwörter der Autor:innen

CMT processHaynes® 282®PWHTadditive manufacturingcooling timemechanical propertiesmicrostructureshielding gas

Autor:innen und Institutionen

  • Institute of Materials and Joining Technology, Otto von Guericke University, 39106 Magdeburg, Germany.
  • Bionic Production GmbH, 21339 Lueneburg, Germany.

ORCID-Profile: Manuela Zinke, Sven Jüttner

Förderung

  • German Association of Joint Industrial Applied Research Institutes
  • German Research Association on Welding and Allied Processes (DVS)
  • AiF (German Federation of Industrial Research Associations)

Zitieren

APA

Zinke, M., Burger, S., & Jüttner, S. (2023). Processing of Haynes® 282® Alloy by Direct Energy Deposition with Arc and Wire. Materials, 16(4), 1715. https://doi.org/10.3390/ma16041715

Vancouver

Zinke M, Burger S, Jüttner S. Processing of Haynes® 282® Alloy by Direct Energy Deposition with Arc and Wire. Materials. 2023;16(4):1715. doi:10.3390/ma16041715

BibTeX
@article{Zinke2023,
  author = {Zinke, Manuela and Burger, Stefan and Jüttner, Sven},
  title = {Processing of Haynes® 282® Alloy by Direct Energy Deposition with Arc and Wire},
  journal = {Materials},
  year = {2023},
  volume = {16},
  number = {4},
  pages = {1715},
  doi = {10.3390/ma16041715}
}
Kostenlos starten →