EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Study on the Layered Structure of Ceramic-Side Bonding Area and the Mechanical Property of Al2O3–Kovar Brazed Joint with Ag-Cu-Ti Filler

Junjie Qi, Dong Du, Dongqi Zhang, Shuai Xue, Jiaming Zhang, Jiamin Yi, Haifei You, Baohua Chang

Journal of Manufacturing and Materials Processing · 29.10.2025 · 9 (11) · 355

DOI: 10.3390/jmmp9110355 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Manufacturing and Materials Processing, online erschienen am 29.10.2025. Verfasst von Junjie Qi und 7 weiteren Autor:innen. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: the Joint Funds of Jiangsu Open bidding for selecting the best candidates.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

During active brazing of alumina ceramics, active elements react with the ceramic to form a reaction layer, which has significant influence on the mechanical property of the brazed joint. However, the composition and formation mechanism of this layer remain unclear among researchers. To fill this gap, different brazing temperatures (900–1100 °C) and heating rates (2.5 °C/min and 10 °C/min) were used to braze 95% Al2O3 ceramics and a Kovar 4J34 alloy using a Ag-Cu-2Ti active brazing filler, and the microstructure and mechanical properties of the joints were investigated. The results show that the joint could be divided into five layers: Al2O3, ceramic-side reaction layer, filler layer, Kovar-side reaction layer, and Kovar. The ceramic-side reaction layer could be further divided into a Ti-O-rich layer and an intermetallics (IMC)-rich layer, and the Kovar-side reaction layer consists of TiFe2 particles, Ag-Cu eutectic, and the remaining Kovar. A belt-like TiFe2+TiNi3 IMC could be found in the filler layer. Increasing the brazing temperature enlarged the belt-like TiFe2+TiNi3 IMC in the filler layer and increased the thickness of the IMC-rich layer in the ceramic-side reaction layer, but had no significant effect on the thickness of the Ti-O-rich layer in the ceramic-side reaction layer. A lower heating rate (2.5 °C/min) was found to suppress the formation of the IMC-rich layer and shift the fracture location in shear tests from the ceramic-side reaction layer to the filler layer, indicating that the strength of the ceramic-side reaction layer was enhanced by controlling the formation of the IMC-rich layer. A maximum shear strength of 170 ± 61 MPa was obtained at a heating rate of 2.5 °C/min and a brazing temperature of 940 °C.

Förderung

  • the Joint Funds of Jiangsu Open bidding for selecting the best candidates

Zitieren

APA

Qi, J., Du, D., Zhang, D., Xue, S., Zhang, J., Yi, J., You, H., & Chang, B. (2025). Study on the Layered Structure of Ceramic-Side Bonding Area and the Mechanical Property of Al2O3–Kovar Brazed Joint with Ag-Cu-Ti Filler. Journal of Manufacturing and Materials Processing, 9(11), 355. https://doi.org/10.3390/jmmp9110355

Vancouver

Qi J, Du D, Zhang D, Xue S, Zhang J, Yi J, et al. Study on the Layered Structure of Ceramic-Side Bonding Area and the Mechanical Property of Al2O3–Kovar Brazed Joint with Ag-Cu-Ti Filler. Journal of Manufacturing and Materials Processing. 2025;9(11):355. doi:10.3390/jmmp9110355

BibTeX
@article{Qi2025,
  author = {Qi, Junjie and Du, Dong and Zhang, Dongqi and Xue, Shuai and Zhang, Jiaming and Yi, Jiamin and You, Haifei and Chang, Baohua},
  title = {Study on the Layered Structure of Ceramic-Side Bonding Area and the Mechanical Property of Al2O3–Kovar Brazed Joint with Ag-Cu-Ti Filler},
  journal = {Journal of Manufacturing and Materials Processing},
  year = {2025},
  volume = {9},
  number = {11},
  pages = {355},
  doi = {10.3390/jmmp9110355}
}
Kostenlos starten →