EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Study on the Synergistic Effects of Pre-Deformation and Post-Aging Treatments on the Mechanical and Corrosion Properties of a 2A97 Al-Cu-Li Alloy

Danyang Liu, Bangguo Wu, Xin Liu, Li Wang, Hua Zhou, Lei Tang, Kefu Gan, Jinfeng Li

Journal of Manufacturing and Materials Processing · 02.07.2026 · 10 (7) · 234

DOI: 10.3390/jmmp10070234 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Manufacturing and Materials Processing, online erschienen am 02.07.2026. Verfasst von Danyang Liu und 7 weiteren Autor:innen. Die Arbeit nennt 52 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Fundamental and Interdisciplinary Disciplines Breakthrough Plan of the Ministry of Education of China, Hunan Youth Science Foundation Project, Key Laboratory Fund for Lightweight and High Strength Material.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This work systematically investigates the effects of pre-deformation, post-aging temperature, and aging time on the mechanical properties, corrosion behavior, and microstructure of a 2A97 Al-Cu-Li alloy. Microstructural characterization indicates that the main precipitates are T1 (Al2CuLi), δ′ (Al3Li), θ′ (Al2Cu), and S′ (Al2CuMg). At 160 °C with 0% pre-deformation strain, increasing aging time increases the size and number density of T1, changing the size and number density of δ′ and θ′ accordingly, whereas raising the aging temperature to 180 °C mainly coarsens precipitates. Increasing pre-deformation from 0% to 12% increases T1 number density and refines its size. Significantly, after aging at 180 °C, θ′ is absent in the 8% and 12% pre-deformed alloys, and T1 re-dissolves in the over-aged 12% alloy. Grain-boundary (GB) phases evolve from fine/discontinuous (under-aged) to fine/continuous (peak-aged) to coarse/discontinuous (over-aged). At the same time, higher pre-strain reduces their size, and higher aging temperature promotes coarsening. Higher aging temperature and pre-deformation accelerate age hardening and shorten the peak-aging time. In the peak-aged state, strength increases but elongation decreases with increasing pre-deformation or aging temperature. Among all, the 4% pre-deformed alloy aged at 160 °C for 30 h shows optimal room-temperature properties, i.e., ultimate tensile strength ~613 MPa, yield strength ~564 MPa, and total elongation ~6.91%. Corrosion resistance was closely related to microstructural evolution during aging, and both prolonged aging and increased pre-deformation decreased the susceptibility to intergranular corrosion. The results provide a basis for optimizing the thermomechanical processing of 2A97 Al-Cu-Li alloys.

Förderung

  • Fundamental and Interdisciplinary Disciplines Breakthrough Plan of the Ministry of Education of China
  • Hunan Youth Science Foundation Project
  • Key Laboratory Fund for Lightweight and High Strength Material

Zitieren

APA

Liu, D., Wu, B., Liu, X., Wang, L., Zhou, H., Tang, L., Gan, K., & Li, J. (2026). Study on the Synergistic Effects of Pre-Deformation and Post-Aging Treatments on the Mechanical and Corrosion Properties of a 2A97 Al-Cu-Li Alloy. Journal of Manufacturing and Materials Processing, 10(7), 234. https://doi.org/10.3390/jmmp10070234

Vancouver

Liu D, Wu B, Liu X, Wang L, Zhou H, Tang L, et al. Study on the Synergistic Effects of Pre-Deformation and Post-Aging Treatments on the Mechanical and Corrosion Properties of a 2A97 Al-Cu-Li Alloy. Journal of Manufacturing and Materials Processing. 2026;10(7):234. doi:10.3390/jmmp10070234

BibTeX
@article{Liu2026,
  author = {Liu, Danyang and Wu, Bangguo and Liu, Xin and Wang, Li and Zhou, Hua and Tang, Lei and Gan, Kefu and Li, Jinfeng},
  title = {Study on the Synergistic Effects of Pre-Deformation and Post-Aging Treatments on the Mechanical and Corrosion Properties of a 2A97 Al-Cu-Li Alloy},
  journal = {Journal of Manufacturing and Materials Processing},
  year = {2026},
  volume = {10},
  number = {7},
  pages = {234},
  doi = {10.3390/jmmp10070234}
}
Kostenlos starten →