EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Microstructural Evolution and Mechanical Behavior of L-PBF Al-Cu 224 Alloy: Role of Process Parameters and Heat Treatment

Esmaeil Pourkhorshid, Paul Rometsch, Mousa Javidani, Alexandre Bily, X.-Grant Chen

Journal of Manufacturing and Materials Processing · 12.06.2026 · 10 (6) · 205

DOI: 10.3390/jmmp10060205 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Manufacturing and Materials Processing, online erschienen am 12.06.2026. Verfasst von Esmaeil Pourkhorshid und 4 weiteren Autor:innen. Die Arbeit nennt 64 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Centre Québécois de Recherche et de Développement de l’Aluminium, Natural Sciences and Engineering Research Council of Canada.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study investigates the effect of laser powder bed fusion (L-PBF) parameters and T7 heat treatment on the defect formation, microstructure, and mechanical properties of a high-strength Al-Cu 224 aluminum alloy. The laser power (200–370 W), scanning speed (130–1900 mm/s), and hatch spacing (90–130 μm) were varied to evaluate their influence on hot cracking and porosity. Microstructural characterization using optical microscopy, scanning electron microscopy, and electron backscatter diffraction revealed that an energy density of 400 J/mm3 substantially reduced visible hot cracking in the examined microscopic regions by reducing the thermal gradients. However, this resulted in increased keyhole porosity, thereby limiting the relative density to 95%. The as-built samples exhibited a yield strength of 152 MPa and an elongation of 9.2%, and the T7 heat treatment improved the yield strength to 233 MPa, whereas the elongation remained unchanged. Keyhole pores served as primary crack initiation/propagation sites during tensile loading, reducing ductility. Lower energy densities increased the geometrically necessary dislocation density and promoted cracking because of higher residual stresses due to greater accumulated plastic strain and lattice curvature. These results clarify process–structure–property relationships, emphasize the trade-offs between defect types and performance, and provide a robust framework for optimizing L-PBF processing of high-strength Al alloys through parameter tuning and post-heat treatment.

Förderung

  • Centre Québécois de Recherche et de Développement de l’Aluminium
  • Natural Sciences and Engineering Research Council of Canada

Zitieren

APA

Pourkhorshid, E., Rometsch, P., Javidani, M., Bily, A., & Chen, X. (2026). Microstructural Evolution and Mechanical Behavior of L-PBF Al-Cu 224 Alloy: Role of Process Parameters and Heat Treatment. Journal of Manufacturing and Materials Processing, 10(6), 205. https://doi.org/10.3390/jmmp10060205

Vancouver

Pourkhorshid E, Rometsch P, Javidani M, Bily A, Chen X. Microstructural Evolution and Mechanical Behavior of L-PBF Al-Cu 224 Alloy: Role of Process Parameters and Heat Treatment. Journal of Manufacturing and Materials Processing. 2026;10(6):205. doi:10.3390/jmmp10060205

BibTeX
@article{Pourkhorshid2026,
  author = {Pourkhorshid, Esmaeil and Rometsch, Paul and Javidani, Mousa and Bily, Alexandre and Chen, X.-Grant},
  title = {Microstructural Evolution and Mechanical Behavior of L-PBF Al-Cu 224 Alloy: Role of Process Parameters and Heat Treatment},
  journal = {Journal of Manufacturing and Materials Processing},
  year = {2026},
  volume = {10},
  number = {6},
  pages = {205},
  doi = {10.3390/jmmp10060205}
}
Kostenlos starten →