Shear Bond Strength of Composite Resin to Carious Primary Dentin After Pretreatment with Silver Diamine Fluoride, Silver Diamine Fluoride–Potassium Iodide or Silver Fluoride–Potassium Iodide: An In Vitro Study
Journal of Functional Biomaterials · 16.11.2026 · 17 (11) · 578
DOI: 10.3390/jfb17110578 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Functional Biomaterials, online erschienen am 16.11.2026. Verfasst von Reem A. Alajlan und 6 weiteren Autor:innen. Die Arbeit nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: King Saud University.
Abstract (Originalsprache)
Silver-based caries-arresting agents are widely used in children, but their effect on the adhesion of composite restorations remains uncertain. This study compared the shear bond strength (SBS) and failure mode of composite resin to carious primary dentin after pretreatment with 38% silver diamine fluoride (SDF), SDF followed by potassium iodide (SDF + KI) or silver fluoride followed by KI (AgF + KI). Forty-eight carious primary molars were randomly allocated to four groups (n = 12). After 24 h in artificial saliva, specimens were etched, bonded and restored with a nanofilled composite. SBS was measured at 0.5 mm/min, and failure modes were classified by two examiners. Mean SBS was 22.79 ± 1.53 MPa (control), 20.85 ± 2.37 MPa (SDF), 15.31 ± 1.74 MPa (SDF + KI) and 12.19 ± 2.09 MPa (AgF + KI) (p < 0.001). Both KI-containing regimens yielded lower SBS than the control and SDF groups (p < 0.001), and AgF + KI was lower than SDF + KI (p = 0.003). SDF alone did not differ significantly from the control (p = 0.115). Failure-mode distribution did not differ significantly among groups. Potassium iodide-containing pretreatments, but not SDF alone, substantially reduced composite adhesion to carious primary dentin.
Förderung
- King Saud University
Zitieren
APA
Alajlan, R. A., AlShathry, A. K., Alabdulmohsen, A. M., Alsaadi, W. E., Aldowsari, M. K., Alshalan, T., & Alshamrani, M. H. (2026). Shear Bond Strength of Composite Resin to Carious Primary Dentin After Pretreatment with Silver Diamine Fluoride, Silver Diamine Fluoride–Potassium Iodide or Silver Fluoride–Potassium Iodide: An In Vitro Study. Journal of Functional Biomaterials, 17(11), 578. https://doi.org/10.3390/jfb17110578
Vancouver
Alajlan RA, AlShathry AK, Alabdulmohsen AM, Alsaadi WE, Aldowsari MK, Alshalan T, et al. Shear Bond Strength of Composite Resin to Carious Primary Dentin After Pretreatment with Silver Diamine Fluoride, Silver Diamine Fluoride–Potassium Iodide or Silver Fluoride–Potassium Iodide: An In Vitro Study. Journal of Functional Biomaterials. 2026;17(11):578. doi:10.3390/jfb17110578
BibTeX
@article{Alajlan2026,
author = {Alajlan, Reem A. and AlShathry, AlJoharah K. and Alabdulmohsen, Amjad M. and Alsaadi, Waad E. and Aldowsari, Mannaa K. and Alshalan, Thakib and Alshamrani, Mohammed H.},
title = {Shear Bond Strength of Composite Resin to Carious Primary Dentin After Pretreatment with Silver Diamine Fluoride, Silver Diamine Fluoride–Potassium Iodide or Silver Fluoride–Potassium Iodide: An In Vitro Study},
journal = {Journal of Functional Biomaterials},
year = {2026},
volume = {17},
number = {11},
pages = {578},
doi = {10.3390/jfb17110578}
}