Polydopamine/SWCNT Ink Functionalization of Silk Fabric to Obtain Electroconductivity at a Low Percolation Threshold
International Journal of Molecular Sciences · 2024
DOI: 10.3390/ijms25095024 ↗Kurz gefasst
Fachartikel in der Zeitschrift International Journal of Molecular Sciences, 2024. Verfasst von Anna Baranowska-Korczyc und 2 weiteren Autor:innen. Beteiligte Einrichtung: Łukasiewicz Research Network-Lodz Institute of Technology, Department of Chemical Textiles Technologies, 9/27 M. Skłodowskiej-Curie Street, 90-570 Lo…. Hauptthemen laut MEDLINE: Indoles, Polymers, Silk, Nanotubes, Carbon. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 40 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Polish Ministry of Science and Higher Education, Ministry of Science and Higher Education, European Union.
Abstract (Originalsprache)
This study presents the functionalization of silk fabric with SWCNT ink. The first step was the formation of a polydopamine (PDA) thin coating on the silk fabric to allow for effective bonding of SWCNTs. PDA formation was carried out directly on the fabric by means of polymerization of dopamine in alkali conditions. The Silk/PDA fabric was functionalized with SWCNT ink of different SWCNT concentrations by using the dip-coating method. IR and Raman analyses show that the dominant β-sheet structure of silk fibroin after the functionalization process remains unchanged. The heat resistance is even slightly improved. The hydrophobic silk fabric becomes hydrophilic after functionalization due to the influence of PDA and the surfactant in SWCNT ink. The ink significantly changes the electrical properties of the silk fabric, from insulating to conductive. The volume resistance changes by nine orders of magnitude, from 2.4 × 1012 Ω to 2.3 × 103 Ω for 0.12 wt.% of SWCNTs. The surface resistance changes by seven orders of magnitude, from 2.1 × 1012 Ω to 2.4 × 105 Ω for 0.17 wt.% of SWCNTs. The volume and surface resistance thresholds are determined to be about 0.05 wt.% and 0.06 wt.%, respectively. The low value of the percolation threshold indicates efficient functionalization, with high-quality ink facilitating the formation of percolation paths through SWCNTs and the influence of the PDA linker.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Łukasiewicz Research Network-Lodz Institute of Technology, Department of Chemical Textiles Technologies, 9/27 M. Skłodowskiej-Curie Street, 90-570 Lodz, Poland.
ORCID-Profile: Anna Baranowska-Korczyc, Małgorzata Cieślak
Förderung
- Polish Ministry of Science and Higher Education
- Ministry of Science and Higher Education
- European Union
- European Regional Development Fund
- National Centre for Research and Development
Zitieren
APA
Baranowska-Korczyc, A., Kowalczyk, D., & Cieślak, M. (2024). Polydopamine/SWCNT Ink Functionalization of Silk Fabric to Obtain Electroconductivity at a Low Percolation Threshold. International Journal of Molecular Sciences. https://doi.org/10.3390/ijms25095024
Vancouver
Baranowska-Korczyc A, Kowalczyk D, Cieślak M. Polydopamine/SWCNT Ink Functionalization of Silk Fabric to Obtain Electroconductivity at a Low Percolation Threshold. International Journal of Molecular Sciences. 2024. doi:10.3390/ijms25095024
BibTeX
@article{BaranowskaKorczyc2024,
author = {Baranowska-Korczyc, Anna and Kowalczyk, Dorota and Cieślak, Małgorzata},
title = {Polydopamine/SWCNT Ink Functionalization of Silk Fabric to Obtain Electroconductivity at a Low Percolation Threshold},
journal = {International Journal of Molecular Sciences},
year = {2024},
doi = {10.3390/ijms25095024}
}
EUVIMED