Tensile and Ablation Properties of Fiber-Reinforced Si-Modified Phenolic Aerogel Composites

Junjie Xu, Hui Gao, Jianlong Chang iD, Lijun Lei iD, Feng Liu, Pengyong Xie, Yuan Cao

Gels · 29.05.2026 · 12 (6) · 473

DOI: 10.3390/gels12060473 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Gels, online erschienen am 29.05.2026. Verfasst von Junjie Xu und 6 weiteren Autor:innen. Beteiligte Einrichtung: School of Mechanical and Electrical Engineering, North University of China, Taiyuan 030051, China. Die Arbeit nennt 44 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Shanxi Scholarship Council of China.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study realizes the synergistic improvement in mechanical properties and ablation resistance of Si-modified phenolic aerogel composites with preserved lightweight characteristics and excellent thermal insulation. The resin matrix forms a uniform nanoporous structure, providing prominent thermal insulation performance. The composite with a fiber density of 0.62 g/cm3 has a low thermal conductivity of 0.086 W/(m·K). The material exhibits reliable tensile strength within a wide temperature range, and its tensile strength rises significantly with an increase in fiber density. The composite with a fiber density of 0.62 g/cm3 delivers a tensile strength of 129 MPa at 20 °C and 102 MPa at 300 °C, which are 79.4% and 122.2% higher than those of the composite with a fiber density of 0.36 g/cm3. In addition, methyltriethoxysilane and quartz fiber knitted felts form in situ SiO2 and SiC ceramic cladding layers under high-temperature ablation, effectively enhancing the ablation resistance of the composites. Higher fiber density greatly reduces the linear ablation rate. With an oxygen flow of 950 L/h and acetylene flow of 700 L/h, the linear ablation rate of the composite with a fiber density of 0.62 g/cm3 is only 0.13 mm/s, 23.1% lower than the composite with a fiber density of 0.36 g/cm3.

Schlagwörter

Stichwörter der Autor:innen

ablation propertiesfiber densitymechanical propertiesnanoporesphenolic aerogel composites

Autor:innen und Institutionen

  • School of Mechanical and Electrical Engineering, North University of China, Taiyuan 030051, China.
  • School of Materials Science and Engineering, North University of China, Taiyuan 030051, China.
  • School of Energy and Power Engineering, North University of China, Taiyuan 030051, China.
  • Naval Research Academy, Beijing 100161, China.

ORCID-Profile: Jianlong Chang, Lijun Lei

Förderung

  • National Natural Science Foundation of China
  • Shanxi Scholarship Council of China

Zitieren

APA

Xu, J., Gao, H., Chang, J., Lei, L., Liu, F., Xie, P., & Cao, Y. (2026). Tensile and Ablation Properties of Fiber-Reinforced Si-Modified Phenolic Aerogel Composites. Gels, 12(6), 473. https://doi.org/10.3390/gels12060473

Vancouver

Xu J, Gao H, Chang J, Lei L, Liu F, Xie P, et al. Tensile and Ablation Properties of Fiber-Reinforced Si-Modified Phenolic Aerogel Composites. Gels. 2026;12(6):473. doi:10.3390/gels12060473

BibTeX
@article{Xu2026,
  author = {Xu, Junjie and Gao, Hui and Chang, Jianlong and Lei, Lijun and Liu, Feng and Xie, Pengyong and Cao, Yuan},
  title = {Tensile and Ablation Properties of Fiber-Reinforced Si-Modified Phenolic Aerogel Composites},
  journal = {Gels},
  year = {2026},
  volume = {12},
  number = {6},
  pages = {473},
  doi = {10.3390/gels12060473}
}
Kostenlos starten →