Kurz gefasst

Fachartikel in der Zeitschrift Fuels, online erschienen am 06.05.2026. Verfasst von Kangkai Xu und 4 weiteren Autor:innen. Die Arbeit nennt 18 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Key R&D Program of China, China National Petroleum Corporation Forward-looking Basic Research Project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Ensuring the integrity of weld seams in pipeline components is critical for the safe and reliable transportation of oil and natural gas. This paper presents a systematic failure investigation of a cracked weld in a reducer located at a natural gas transmission station in Western China, aiming to identify the failure mechanism and assess its implications for pipeline safety management. A comprehensive analysis was conducted using macroscopic examination, chemical composition analysis, mechanical property testing, metallographic observation, and microscopic fracture characterization. The results reveal that the heat-affected zone (HAZ) exhibited abnormally high hardness (up to 588 HV0.1), indicating insufficient toughness that made it susceptible to cracking. The base metal showed a high carbon equivalent (CEV), placing it in the “difficult-to-weld” category and increasing its sensitivity to improper welding thermal cycles. On-site investigation further identified significant deficiencies in welding process control, including inadequate preheating, improper interpass temperature management, and insufficient post-weld heat treatment (PWHT). These deficiencies allowed welding residual stresses to persist and failed to mitigate the hardened HAZ microstructure. The combination of poor material weldability and inadequate on-site welding practices ultimately led to brittle fracture under service conditions. This failure highlights a critical vulnerability in pipeline transportation infrastructure and underscores the necessity of strict adherence to qualified welding procedures for high-carbon-equivalent steels. The findings provide practical guidance for enhancing welding quality control and ensuring the long-term operational safety of natural gas pipeline systems.

Förderung

  • National Key R&D Program of China
  • China National Petroleum Corporation Forward-looking Basic Research Project

Zitieren

APA

Xu, K., Wang, P., Wang, S., Xie, S., & Wang, B. (2026). Weld Seam Failure Analysis of a Natural Gas Pipeline Reducer: Implications for Oil and Gas Transportation Safety. Fuels, 7(2), 30. https://doi.org/10.3390/fuels7020030

Vancouver

Xu K, Wang P, Wang S, Xie S, Wang B. Weld Seam Failure Analysis of a Natural Gas Pipeline Reducer: Implications for Oil and Gas Transportation Safety. Fuels. 2026;7(2):30. doi:10.3390/fuels7020030

BibTeX
@article{Xu2026,
  author = {Xu, Kangkai and Wang, Peng and Wang, Shuai and Xie, Shuyi and Wang, Bohong},
  title = {Weld Seam Failure Analysis of a Natural Gas Pipeline Reducer: Implications for Oil and Gas Transportation Safety},
  journal = {Fuels},
  year = {2026},
  volume = {7},
  number = {2},
  pages = {30},
  doi = {10.3390/fuels7020030}
}
Kostenlos starten →