Kurz gefasst

Fachartikel in der Zeitschrift Eng, online erschienen am 01.06.2026. Verfasst von Linghai Kong und 5 weiteren Autor:innen. Die Arbeit nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Science and Technology Innovation Program of Hunan Province, Education Department Research Foundation of Hunan Province, Natural Science Foundation of Hunan Province of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Ultra-high performance concrete (UHPC) is widely used for its excellent compactness and durability. However, steel fibers in UHPC may form conductive paths, affecting electrochemical testing of internal rebars. To assess the applicability of current testing standards in UHPC, specimens of UHPC, high-performance concrete (HPC), and normal concrete (NC) with different cover thicknesses are designed. Open circuit potential (OCP), linear polarization resistance (LPR), and Tafel polarization curves are adopted to compare the corrosion behavior during 180 days of chloride immersion. Results show that UHPC has the most negative OCP, followed by NC and HPC. According to ASTM C876, this would indicate the highest corrosion risk for UHPC, contradicting its well-known superior chloride resistance. Hence, ASTM C876 is not applicable to UHPC. Corrosion current density (Icorr) is smallest in UHPC, followed by HPC and NC, consistent with chloride resistance ranking, indicating good applicability of the linear polarization method to UHPC. The anodic Tafel slope is larger than the cathodic one for all specimens, showing anodic control, unaffected by steel fibers. Larger cover thickness leads to higher OCP, higher polarization resistance, and lower Icorr. At 30 mm cover, internal rebars in UHPC are essentially non-corroded.

Förderung

  • Science and Technology Innovation Program of Hunan Province
  • Education Department Research Foundation of Hunan Province
  • Natural Science Foundation of Hunan Province of China

Zitieren

APA

Kong, L., Li, G., Agudamu, He, X., Luo, Z., & Zhang, X. (2026). Applicability of Electrochemical Testing for Internal Steel Rebar Corrosion in UHPC Under Chloride Environment. Eng, 7(6), 265. https://doi.org/10.3390/eng7060265

Vancouver

Kong L, Li G, Agudamu, He X, Luo Z, Zhang X. Applicability of Electrochemical Testing for Internal Steel Rebar Corrosion in UHPC Under Chloride Environment. Eng. 2026;7(6):265. doi:10.3390/eng7060265

BibTeX
@article{Kong2026,
  author = {Kong, Linghai and Li, Gen and Agudamu and He, Xunlin and Luo, Zhengdong and Zhang, Xuhui},
  title = {Applicability of Electrochemical Testing for Internal Steel Rebar Corrosion in UHPC Under Chloride Environment},
  journal = {Eng},
  year = {2026},
  volume = {7},
  number = {6},
  pages = {265},
  doi = {10.3390/eng7060265}
}
Kostenlos starten →