High-voltage direct-current submarine cables operate under coupled electrical and thermal stresses. Radial temperature gradients may induce non-uniform aging and space charge accumulation in XLPE insulation. This study compares uniformly aged XLPE film specimens with radial slices taken from a full-size ±500 kV HVDC submarine cable aged under a temperature gradient. Uniform thermal aging was conducted at 100 °C and 135 °C for 1176 h. For the full-size cable, the heating-side boundary was maintained at 135 ± 1 °C, while the outer cable surface was maintained at approximately 100 °C by forced-air cooling. This established a nominal radial boundary-temperature difference of approximately 35 °C. After aging, 500 μm-thick specimens were sliced from different radial positions. Their space charge distributions were measured using the pulsed electro-acoustic (PEA) method under a DC field of −40 kV/mm. Electric-field distributions, average bulk charge densities, and electric-field distortion rates were evaluated, together with the charge retention characteristics during depolarization. DC volume conductivity was also measured to assess changes in electrical conduction. The results indicate that space charge accumulation in uniformly aged specimens does not increase monotonically with aging temperature. In contrast, the conductor-side slice from the temperature-gradient-aged cable shows pronounced heterocharge accumulation, severe local electric-field distortion, and slower residual charge dissipation. Its electric-field distortion rate reaches 167.6%. Its average bulk charge density also remains much higher than those of the other specimens during depolarization. These findings demonstrate that temperature-gradient aging in full-size cables cannot be represented by uniform aging of XLPE film specimens.
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Zhu, W., Hui, B., Fan, L., Li, Y., Tian, Z., Han, T., Yang, H., & Chu, J. (2026). A Comparative Study of Space Charge Characteristics in Uniformly Aged XLPE Film Specimens and Radial Slices from a Full-Size HVDC Cable. Energies, 19(22), 5559. https://doi.org/10.3390/en19225559
Vancouver
Zhu W, Hui B, Fan L, Li Y, Tian Z, Han T, et al. A Comparative Study of Space Charge Characteristics in Uniformly Aged XLPE Film Specimens and Radial Slices from a Full-Size HVDC Cable. Energies. 2026;19(22):5559. doi:10.3390/en19225559
BibTeX
@article{Zhu2026,
author = {Zhu, Wenbo and Hui, Baojun and Fan, Lingmeng and Li, Yanfei and Tian, Zhengbing and Han, Tao and Yang, Heng and Chu, Jia},
title = {A Comparative Study of Space Charge Characteristics in Uniformly Aged XLPE Film Specimens and Radial Slices from a Full-Size HVDC Cable},
journal = {Energies},
year = {2026},
volume = {19},
number = {22},
pages = {5559},
doi = {10.3390/en19225559}
}
EUVIMED