EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Microbial Biofilm Reduces the Strength Reliability of 3D-Printed Appliance Resins

Watt Sook May, Ng Zicong iD, Vinicius Rosa iD, Kelvin Weng Chiong Foong

Dentistry Journal · 05.08.2026 · 14 (8) · 487

DOI: 10.3390/dj14080487 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Dentistry Journal, online erschienen am 05.08.2026. Verfasst von Watt Sook May und 3 weiteren Autor:innen. Beteiligte Einrichtung: Faculty of Dentistry, National University of Singapore, 9 Lower Kent Ridge Road, Singapore 119085, Singapore. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 28 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National University of Singapore, Singapore Ministry of Education.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Background/Objectives: Three-dimensionally (3D) printed resins are increasingly used for removable orthodontic appliances, but how their mechanical reliability changes in the oral environment is unclear. This study evaluated the effect of bio-ageing environment and material type on the biaxial flexural strength and Weibull reliability of one conventional acrylic resin (Orthocryl, OC) and two 3D-printed photopolymer resins (BioMed Clear, BMC; and KeySplint Hard, KH). The Weibull modulus (m) reflects how consistent, or predictable, the strength is among specimens, independent of its average value.

Methods

Disc specimens (n = 32) were aged for 24 h at 37 °C in pooled human saliva, a Streptococcus mutans biofilm, or water, and the biaxial flexural strength was measured by the piston-on-three-balls method (1 mm/min). Data were analysed with two- and three-parameter Weibull statistics to estimate the Weibull modulus (m), characteristic strength (σ0), strength at 5% failure probability (σ5%), and threshold strength (σμ), with model selection guided by the Akaike Information Criterion.

Results

Biofilm exposure lowered m while σ0 was preserved: m fell from 9.96 (saliva) and 7.98 (water) to 1.95 for OC, and from 17.61 and 13.01 to 2.62 for BMC, whereas σ0 stayed near 55 MPa (OC) and 64 MPa (BMC). Under biofilm the modulus of all three converged to low values (1.4–2.6), abolishing the differences among materials; OC and BMC required a three-parameter model only after biofilm (σu ≈ 41 MPa), whereas KH required it in every environment (σu = 28.9–38.7 MPa).

Conclusions

Biofilm ageing mainly reduced strength predictability, while characteristic strength was largely preserved. This indicates that flexural strength alone may be insufficient to qualify resins for removable appliances, and that printed resins studied here are not inherently superior or inferior to conventional acrylic.

Schlagwörter

Stichwörter der Autor:innen

acrylic resinsbiofilmsflexural strengthmaterials testingprintingthree-dimensional

Autor:innen und Institutionen

  • Faculty of Dentistry, National University of Singapore, 9 Lower Kent Ridge Road, Singapore 119085, Singapore.

ORCID-Profile: Ng Zicong, Vinicius Rosa

Förderung

  • National University of Singapore
  • Singapore Ministry of Education

Zitieren

APA

May, W. S., Zicong, N., Rosa, V., & Foong, K. W. C. (2026). Microbial Biofilm Reduces the Strength Reliability of 3D-Printed Appliance Resins. Dentistry Journal, 14(8), 487. https://doi.org/10.3390/dj14080487

Vancouver

May WS, Zicong N, Rosa V, Foong KWC. Microbial Biofilm Reduces the Strength Reliability of 3D-Printed Appliance Resins. Dentistry Journal. 2026;14(8):487. doi:10.3390/dj14080487

BibTeX
@article{May2026,
  author = {May, Watt Sook and Zicong, Ng and Rosa, Vinicius and Foong, Kelvin Weng Chiong},
  title = {Microbial Biofilm Reduces the Strength Reliability of 3D-Printed Appliance Resins},
  journal = {Dentistry Journal},
  year = {2026},
  volume = {14},
  number = {8},
  pages = {487},
  doi = {10.3390/dj14080487}
}
Kostenlos starten →