EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Crystal Evolution and Optical Properties of Sr1−xNixTiO3 Solid Solutions Prepared via Coprecipitated-Hydrothermal Processing

Jorge Cisneros-Preciado, Juan Carlos Rendón-Angeles, Zully Matamoros-Veloza, Jorge López-Cuevas, Tadaharu Ueda, Tomai Takaaki

Crystals · 20.11.2026 · 16 (11) · 739

DOI: 10.3390/cryst16110739 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Crystals, online erschienen am 20.11.2026. Verfasst von Jorge Cisneros-Preciado und 5 weiteren Autor:innen. Die Arbeit nennt 50 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: The Centre for Research and Advanced Studies.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Soft-chemical processing combining gel coprecipitation and hydrothermal synthesis to prepare Sr1−xNixTiO3 and Ni1−x SrxTiO3 solid solutions (SS1 and SS1*) was investigated. SS1 with pseudocubic symmetry crystallised with 0.0–23.8 mol% Ni2+ at 200 °C for 6 h; at 34.7–72.7 mol% Ni2+, intermediate Sr1−xNixTiO3 (SS1*, 34.7–53.7 mol% Ni2+) and Ni-rich Ni1−x SrxTiO3 (SS1*, 53.7–72.7 mol% Ni2+) both crystallised with pseudo-orthorhombic symmetry, accommodating Ni2+ at the perovskite A-site. At higher Ni2+ contents, NiTiO3 (SS2) preferentially crystallised and coexisted with secondary NiTi3O7. Increasing the hydrothermal temperature to 240 °C destabilised the pseudo-orthorhombic phase, whereas prolonged treatment of Sr0.5Ni0.5TiO3 at 200 °C promoted NiTi3O7 formation. SS1 powders with up to 23.8 mol% Ni2+ formed pseudocuboidal particles averaging about 260 nm, whereas SS1* powders comprised irregular clusters of primary crystallites averaging about 8.5 nm. Diffuse reflectance decreased from 75.2% for SrTiO3 to 48.6% for SS1* powders, while the calculated near-infrared (NIR, 780–2500 nm) solar reflectance ranged from 44.31% to 66.51%. Ni2+ incorporation induced an absorption band at 544 nm in the Ni1−x SrxTiO3 SS1* powders and reduced the “Bg” from 3.20 eV (SrTiO3) to 2.41 eV (Ni-rich SS1*). Soft-chemical processing thus tunes phase stability, particle morphology, and optical properties, supporting SrTiO3–NiTiO3 solid solutions as cool pigments and candidate photocatalysts.

Förderung

  • The Centre for Research and Advanced Studies

Zitieren

APA

Cisneros-Preciado, J., Rendón-Angeles, J. C., Matamoros-Veloza, Z., López-Cuevas, J., Ueda, T., & Takaaki, T. (2026). Crystal Evolution and Optical Properties of Sr1−xNixTiO3 Solid Solutions Prepared via Coprecipitated-Hydrothermal Processing. Crystals, 16(11), 739. https://doi.org/10.3390/cryst16110739

Vancouver

Cisneros-Preciado J, Rendón-Angeles JC, Matamoros-Veloza Z, López-Cuevas J, Ueda T, Takaaki T. Crystal Evolution and Optical Properties of Sr1−xNixTiO3 Solid Solutions Prepared via Coprecipitated-Hydrothermal Processing. Crystals. 2026;16(11):739. doi:10.3390/cryst16110739

BibTeX
@article{CisnerosPreciado2026,
  author = {Cisneros-Preciado, Jorge and Rendón-Angeles, Juan Carlos and Matamoros-Veloza, Zully and López-Cuevas, Jorge and Ueda, Tadaharu and Takaaki, Tomai},
  title = {Crystal Evolution and Optical Properties of Sr1−xNixTiO3 Solid Solutions Prepared via Coprecipitated-Hydrothermal Processing},
  journal = {Crystals},
  year = {2026},
  volume = {16},
  number = {11},
  pages = {739},
  doi = {10.3390/cryst16110739}
}
Kostenlos starten →