EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Spheroidization Behavior of TiZrNbTa Refractory High-Entropy Alloy Powder During Radio Frequency Plasma Processing

Xingyi Chen, Yi Zhang, Zhihua Zhuang, Jinyan He, Hao Chen, Wenlian Peng, Xinggao Zhang, Wenchao Zhu, Hanqing Xu, Liang Zhou

Crystals · 02.11.2026 · 16 (11) · 701

DOI: 10.3390/cryst16110701 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Crystals, online erschienen am 02.11.2026. Verfasst von Xingyi Chen und 9 weiteren Autor:innen. Die Arbeit nennt 26 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Spherical TiZrNbTa refractory high-entropy alloy powders with uniform composition and good flowability are essential feedstock for powder-based additive manufacturing; however, irregular powders produced by the hydrogenation-dehydrogenation route generally require further shaping treatment. Radio frequency (RF) plasma spheroidization of TiZrNbTa refractory high-entropy alloy powders prepared by hydrogenation-dehydrogenation (HDH) was investigated at a fixed power of 12 kW. Fine (10–40 μm) and coarse (40–70 μm) powders were compared at 5.0 g/min, followed by feed-rate tests (2.5–7.5 g/min) on the coarse fraction. At 5.0 g/min, the spheroidization degrees of the fine and coarse powders were 45.33% and 50.88%, respectively. The fine powder exhibited satellite particles and a broadened particle-size distribution, whereas the coarse powder retained some irregular particles. Decreasing the coarse-powder feed rate from 7.5 to 2.5 g/min increased the spheroidization degree from 45.71% to 94.55%, with median particle size (D50) reaching 56.84 μm and a narrower particle-size distribution. The powders retained predominantly body-centered cubic (BCC) diffraction signatures, while dendritic substructures and local Ta/Zr segregation varied with processing conditions. Testing showed that untreated coarse HDH powder did not flow unaided through a Hall funnel, whereas the 5.0 g/min spheroidized product flowed in 18.7 s/50 g; after spheroidization, its loose bulk density increased from 4.68 to 5.47 g/cm3. These results clarify the effects of particle size and powder feed rate on spheroidization behavior within the investigated conditions.

Zitieren

APA

Chen, X., Zhang, Y., Zhuang, Z., He, J., Chen, H., Peng, W., Zhang, X., Zhu, W., Xu, H., & Zhou, L. (2026). Spheroidization Behavior of TiZrNbTa Refractory High-Entropy Alloy Powder During Radio Frequency Plasma Processing. Crystals, 16(11), 701. https://doi.org/10.3390/cryst16110701

Vancouver

Chen X, Zhang Y, Zhuang Z, He J, Chen H, Peng W, et al. Spheroidization Behavior of TiZrNbTa Refractory High-Entropy Alloy Powder During Radio Frequency Plasma Processing. Crystals. 2026;16(11):701. doi:10.3390/cryst16110701

BibTeX
@article{Chen2026,
  author = {Chen, Xingyi and Zhang, Yi and Zhuang, Zhihua and He, Jinyan and Chen, Hao and Peng, Wenlian and Zhang, Xinggao and Zhu, Wenchao and Xu, Hanqing and Zhou, Liang},
  title = {Spheroidization Behavior of TiZrNbTa Refractory High-Entropy Alloy Powder During Radio Frequency Plasma Processing},
  journal = {Crystals},
  year = {2026},
  volume = {16},
  number = {11},
  pages = {701},
  doi = {10.3390/cryst16110701}
}
Kostenlos starten →