Fachartikel in der Zeitschrift Crystals, online erschienen am 18.06.2026. Verfasst von He Guo und 7 weiteren Autor:innen. Die Arbeit nennt 36 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Rare Earth New Material Technology Innovation Center Open Subject Project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Mg–Y–Zn alloys have attracted considerable attention for lightweight structural applications; however, the influence of extrusion temperature on microstructural evolution and the underlying mechanisms governing strength–ductility synergy remains insufficiently understood. In this study, a novel YZG921 (Mg–9Y–1.8Zn–1.2Gd–0.5Zr–0.3Ca, wt.%) alloy was fabricated by hot extrusion at temperatures ranging from 480 to 520 °C. The microstructure, mechanical properties, and deformation behavior were systematically investigated using SEM, TEM, EBSD, in situ EBSD, and slip-trace analysis. The results show that extrusion temperature significantly affects the evolution of secondary phases, grain size, and texture intensity. At 500 °C, an 18R-LPSO phase was formed, accompanied by a more homogeneous distribution of secondary phases and the finest grain structure (~3.8 μm), whereas the average grain size remained close to 10 μm for the alloys extruded at 480 °C and 520 °C. Meanwhile, the maximum basal texture intensity decreased from 4.16 to 4.79 m.r.d. to 2.18–2.58 m.r.d. Mechanical testing revealed that the alloy extruded at 500 °C exhibited the optimum strength–ductility balance, with an ultimate tensile strength of 498.4 MPa and an elongation of 13.8%. In situ EBSD analysis showed that the fraction of low-angle grain boundaries increased from ~7% to 43% during tensile deformation, while the average KAM value increased from ~0.5° to 0.88°. Slip-trace analysis further demonstrated that plastic deformation was predominantly governed by basal slip, accounting for approximately 84.2% of the activated slip systems. The superior mechanical performance achieved at 500 °C is attributed to the synergistic effects of grain refinement, LPSO and second-phase strengthening, texture weakening, and sustained strain hardening. These findings provide insights into microstructure–property relationships and offer guidance for the optimization of thermomechanical processing parameters in Mg–Y–Zn alloys.

Förderung

  • Rare Earth New Material Technology Innovation Center Open Subject Project

Zitieren

APA

Guo, H., Hu, W., Wang, W., Liu, F., He, W., Yu, Z., Wang, X., & Lu, Y. (2026). Effect of Deformation Process on Mechanical Properties of Hot-Extruded Mg-Y-Zn-Gd-Zr-Ca Alloy. Crystals, 16(6), 397. https://doi.org/10.3390/cryst16060397

Vancouver

Guo H, Hu W, Wang W, Liu F, He W, Yu Z, et al. Effect of Deformation Process on Mechanical Properties of Hot-Extruded Mg-Y-Zn-Gd-Zr-Ca Alloy. Crystals. 2026;16(6):397. doi:10.3390/cryst16060397

BibTeX
@article{Guo2026,
  author = {Guo, He and Hu, Wenxin and Wang, Wei and Liu, Feng and He, Wei and Yu, Zemin and Wang, Xinyuan and Lu, Yuming},
  title = {Effect of Deformation Process on Mechanical Properties of Hot-Extruded Mg-Y-Zn-Gd-Zr-Ca Alloy},
  journal = {Crystals},
  year = {2026},
  volume = {16},
  number = {6},
  pages = {397},
  doi = {10.3390/cryst16060397}
}
Kostenlos starten →