Heat Treatment Post-Processing for the Improved Mechanical Properties of Scalmalloy® Processed via Directed Energy Deposition
Crystals · 27.07.2024 · 14 (8) · 688
DOI: 10.3390/cryst14080688 ↗Kurz gefasst
Fachartikel in der Zeitschrift Crystals, online erschienen am 27.07.2024. Verfasst von Rachel Boillat-Newport und 2 weiteren Autor:innen. Die Arbeit wurde bisher 9-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: DoEdu GAANN, NSF, Product Innovation and Engineering, LLC..
Abstract (Originalsprache)
As high-strength aluminum alloys present several processability issues with additive manufacturing (AM), Scalmalloy®, an Al-Mg-Sc-Zr-based alloy, has been developed. This alloy is age-hardenable, allowing it to precipitate out a strengthening precipitate phase, Al3(Sc,Zr). The manufacturer recommends a single-stage aging treatment at 325 °C for 4 h; however, the majority of the literature studies utilize a powder bed processing known as selective laser melting (SLM) over powder-fed processing directed energy deposition (DED). This study addresses the lack of information on heat treatments for DED fabrication by exploring the application of artificial aging temperatures of 300–400 °C for 2, 4, and 6 h to: 1. determine the impact on the microstructural evolution and mechanical performance and 2. determine whether the recommended treatment for Scalmalloy® is appropriate for DED fabrication. Tensile testing determined that low-temperature treatments exhibited no visible dependence on time (2–6 h); however, time becomes influential at higher temperatures starting at 350 °C. The temperature plays a considerable role in the mechanical and microstructural behaviors of DED Scalmalloy®. The highest tensile strength was noted at 300 °C (384 MPa, 21.6% increase), but all heat-treated cases resulted in an improvement over the as-built case. This investigation established that increasing the treatment temperature resulted in a decreasing trend for the tensile strength that held over time. Elongation at 2 h displayed a near parabolic trend that peaks at 350 °C (20%) and falls with higher temperatures. At the 4 h treatment, a slight decreasing trend was noticed for elongation. No visible change was observed for elongation at 6 h, with elongation values remaining fairly consistent. The microstructural evolution, including micron-sized and nano-sized Al3(Sc,Zr) and grain size, was examined, and coarsening effects were noted with the increase in the temperature. It is recommended that treatment be conducted at 300 °C to achieve the precipitation of the strengthening Al3(Sc,Zr) phase while minimizing coarsening.
Förderung
- DoEdu GAANN
- NSF
- Product Innovation and Engineering, LLC.
Zitieren
APA
Boillat-Newport, R., Isanaka, S. P., & Liou, F. (2024). Heat Treatment Post-Processing for the Improved Mechanical Properties of Scalmalloy® Processed via Directed Energy Deposition. Crystals, 14(8), 688. https://doi.org/10.3390/cryst14080688
Vancouver
Boillat-Newport R, Isanaka SP, Liou F. Heat Treatment Post-Processing for the Improved Mechanical Properties of Scalmalloy® Processed via Directed Energy Deposition. Crystals. 2024;14(8):688. doi:10.3390/cryst14080688
BibTeX
@article{BoillatNewport2024,
author = {Boillat-Newport, Rachel and Isanaka, Sriram Praneeth and Liou, Frank},
title = {Heat Treatment Post-Processing for the Improved Mechanical Properties of Scalmalloy® Processed via Directed Energy Deposition},
journal = {Crystals},
year = {2024},
volume = {14},
number = {8},
pages = {688},
doi = {10.3390/cryst14080688}
}