Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes
Construction Materials · 17.11.2026 · 6 (6) · 107
DOI: 10.3390/constrmater6060107 ↗Kurz gefasst
Fachartikel in der Zeitschrift Construction Materials, online erschienen am 17.11.2026. Verfasst von Samantha R. Doughty und 6 weiteren Autor:innen. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Novaphos.
Abstract (Originalsprache)
The phosphate fertilizer industry generates large quantities of phosphogypsum, motivating beneficial-use pathways that convert phosphate-industry residuals into construction materials. This study evaluated calcium silicate-rich J-Rox co-products produced through two source routes: phosphate ore-derived J-Rox from the phosphoric acid production route (JR-P) and phosphogypsum-derived J-Rox from the phosphogypsum recovery route (JR-G). Finely ground J-Rox was examined as a supplementary cementitious material through a staged paste–mortar–concrete framework, while coarsely ground phosphogypsum-derived J-Rox sand was evaluated as a prewetted internal curing aggregate. Paste testing assessed setting behavior, mortar testing evaluated workability-controlled compressive strength and sulfate attack resistance, and concrete testing validated JR-G materials (JR-G1 and JR-G2) in binary, ternary J-Rox–slag, and internally cured systems. JR-P materials produced more systematic setting delay, likely influenced by higher P2O5 contents, while JR-G materials showed more variable but practical setting behavior. Mortar strength results were material- and dosage-dependent, with 15% replacement giving the most consistent response. Sulfate expansion provided the clearest source-route distinction: all JR-G mixtures remained below the 0.1% expansion threshold at 26 weeks, with an average expansion of 0.0560%, while five of the six JR-P mixtures exceeded this threshold, with an average expansion of 0.1499%. At the concrete scale, binary JR-G mixtures achieved practical 28-day strength, with the 15JR-G2 mixture reaching 7593 psi at 91 days compared with 6694 psi for the OPC control. Ternary mixtures containing 15% JR-G and 35% slag showed strong later-age strength gain, increased surface resistivity, and reduced drying shrinkage at 50% OPC replacement. Specifically, the 15JR-G2/35S mixture achieved a 91-day compressive strength of 7372 psi, while the 15JR-G1/35S mixture exhibited a 112-day drying shrinkage of −0.011%, compared with −0.066% for the OPC control. These results indicate that phosphogypsum-derived J-Rox use in concrete materials shows promise, particularly when used in ternary, performance-engineered blended binder systems.
Förderung
- Novaphos
Zitieren
APA
Doughty, S. R., Mishra, S., Summers, C. J., Tempest, B. Q., Armaghani, J., Vignovic, M., & Cavalline, T. L. (2026). Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes. Construction Materials, 6(6), 107. https://doi.org/10.3390/constrmater6060107
Vancouver
Doughty SR, Mishra S, Summers CJ, Tempest BQ, Armaghani J, Vignovic M, et al. Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes. Construction Materials. 2026;6(6):107. doi:10.3390/constrmater6060107
BibTeX
@article{Doughty2026,
author = {Doughty, Samantha R. and Mishra, Shubham and Summers, Clarke J. and Tempest, Brett Q. and Armaghani, Jamshid and Vignovic, Mark and Cavalline, Tara L.},
title = {Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes},
journal = {Construction Materials},
year = {2026},
volume = {6},
number = {6},
pages = {107},
doi = {10.3390/constrmater6060107}
}