EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

High-Temperature Corrosion Mechanisms of La2Si2O7 Environmental Barrier Coatings Exposed to Molten Calcium–Magnesium–Aluminosilicate (CMAS) and Water Vapor/Oxygen

Wei Zhang, Jie Xia, Ling Zhang, Xianyang Zeng, Jinhui Zhao, Yiqi Xiao, Zhi Wu

Coatings · 11.08.2026 · 16 (8) · 950

DOI: 10.3390/coatings16080950 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Coatings, online erschienen am 11.08.2026. Verfasst von Wei Zhang und 6 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Key Laboratory of Low Dimensional Materials and Application Technology (Xiangtan University) of the Ministry of Education, Characteristic Application Discipline of Material Science and Engineering in Hunan Province, Scientific Research Project of Hunan Institute of Technology.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

La2Si2O7 is a candidate environmental barrier coating (EBC) material for silicon carbide ceramic matrix composites in next-generation gas turbine engines, yet its degradation behavior under the simultaneous attack of molten CMAS and water vapor remains insufficiently understood. This study systematically examines atmospheric plasma-sprayed La2Si2O7 coatings exposed to four environments (air, CMAS alone, H2O/O2 alone, and combined CMAS + H2O/O2) at 1400 °C for 8 h. Under dry air, the coating recrystallizes to La2Si2O7 with negligible corrosion. CMAS attack triggers a dissolution–reprecipitation mechanism forming needle-like CaLa4(SiO4)3O apatite within a denser reaction zone, which partially impedes further infiltration. Water vapor accelerated the growth of the thermally grown oxide at the bond coat interface. The combined CMAS + H2O/O2 environment produced a pronounced synergistic acceleration: water vapor reduced CMAS melt viscosity, enabling deeper CMAS penetration, while concurrent silica volatilization disrupted the protective apatite barrier, generating extensive porosity and through-coating cracking. These findings reveal that the inherent CMAS resistance of La2Si2O7 via apatite formation is critically compromised by simultaneous water vapor, highlighting a key challenge for its application in realistic engine environments.

Förderung

  • Key Laboratory of Low Dimensional Materials and Application Technology (Xiangtan University) of the Ministry of Education
  • Characteristic Application Discipline of Material Science and Engineering in Hunan Province
  • Scientific Research Project of Hunan Institute of Technology

Zitieren

APA

Zhang, W., Xia, J., Zhang, L., Zeng, X., Zhao, J., Xiao, Y., & Wu, Z. (2026). High-Temperature Corrosion Mechanisms of La2Si2O7 Environmental Barrier Coatings Exposed to Molten Calcium–Magnesium–Aluminosilicate (CMAS) and Water Vapor/Oxygen. Coatings, 16(8), 950. https://doi.org/10.3390/coatings16080950

Vancouver

Zhang W, Xia J, Zhang L, Zeng X, Zhao J, Xiao Y, et al. High-Temperature Corrosion Mechanisms of La2Si2O7 Environmental Barrier Coatings Exposed to Molten Calcium–Magnesium–Aluminosilicate (CMAS) and Water Vapor/Oxygen. Coatings. 2026;16(8):950. doi:10.3390/coatings16080950

BibTeX
@article{Zhang2026,
  author = {Zhang, Wei and Xia, Jie and Zhang, Ling and Zeng, Xianyang and Zhao, Jinhui and Xiao, Yiqi and Wu, Zhi},
  title = {High-Temperature Corrosion Mechanisms of La2Si2O7 Environmental Barrier Coatings Exposed to Molten Calcium–Magnesium–Aluminosilicate (CMAS) and Water Vapor/Oxygen},
  journal = {Coatings},
  year = {2026},
  volume = {16},
  number = {8},
  pages = {950},
  doi = {10.3390/coatings16080950}
}
Kostenlos starten →