Fachartikel in der Zeitschrift Coatings, online erschienen am 18.05.2026. Verfasst von Zhongying Liu und 3 weiteren Autor:innen. Die Arbeit nennt 32 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Henan Provincial Key Research and Development Program Project, Henan International Science and Technology Cooperation Project.
Abstract (Originalsprache)
Dissimilar 7075-T6 and 6061-T6 aluminum alloy joints were fabricated using pulsed metal inert gas (P-MIG) welding with ER5356 filler wire. The effects of welding current (224 A, 234 A, and 244 A) on macro-morphology, microstructure, mechanical properties, and corrosion behavior were systematically investigated. As welding current increased, the top and bottom reinforcements first increased and then decreased, reaching maximum values at 234 A, while the front weld width exhibited the opposite trend. The weld zone consisted of equiaxed and dendritic grains, with partial remelting of AlFeMnSi intermetallic compounds observed in the heat-affected zones. The microhardness and tensile strength of the joints followed a similar trend of first decreasing and then increasing with welding current, achieving a maximum tensile strength of 203.9 MPa at 244 A, corresponding to 89.5% of the 6061-T6 base metal strength. Corrosion resistance varied across regions depending on the evaluation method. In intergranular corrosion tests, the 7075-HAZ showed the highest susceptibility due to grain boundary segregation of Mg and Zn. In electrochemical tests, the WZ exhibited the poorest corrosion resistance. For the 7075-HAZ, optimal corrosion resistance was achieved at 234 A, attributed to a stable passive film and uniform precipitate distribution. These findings provide valuable guidance for optimizing P-MIG welding parameters for dissimilar 7075/6061 aluminum alloy joints.
Förderung
- National Natural Science Foundation of China
- Henan Provincial Key Research and Development Program Project
- Henan International Science and Technology Cooperation Project
- Science & Technology Innovation Talents in Universities of Henan Province
- Henan Provincial Foreign Experts Program
Zitieren
APA
Liu, Z., Liu, L., Li, S., & Du, S. (2026). Effect of Welding Current on Microstructure and Properties of 7075/6061 Aluminum Alloy Dissimilar Pulsed MIG Welded Joints. Coatings, 16(5), 608. https://doi.org/10.3390/coatings16050608
Vancouver
Liu Z, Liu L, Li S, Du S. Effect of Welding Current on Microstructure and Properties of 7075/6061 Aluminum Alloy Dissimilar Pulsed MIG Welded Joints. Coatings. 2026;16(5):608. doi:10.3390/coatings16050608
BibTeX
@article{Liu2026,
author = {Liu, Zhongying and Liu, Linjun and Li, Shuai and Du, Sanming},
title = {Effect of Welding Current on Microstructure and Properties of 7075/6061 Aluminum Alloy Dissimilar Pulsed MIG Welded Joints},
journal = {Coatings},
year = {2026},
volume = {16},
number = {5},
pages = {608},
doi = {10.3390/coatings16050608}
}
EUVIMED