Failure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment

Wenhui Yang, Rende Mu, Limin He, Shuai Li, Huangyue Cai, Delin Liu

Coatings · 09.05.2026 · 16 (5) · 574

DOI: 10.3390/coatings16050574 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Coatings, online erschienen am 09.05.2026. Verfasst von Wenhui Yang und 5 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 48 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Beijing Institute of Aeronautical Materials.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To simulate the erosion damage behavior of thermal barrier coatings (TBCs) under actual service conditions in an aircraft engine environment, this study developed a multi-factor coupled test setup capable of simulating combined loading under high-temperature (1150 °C), high-speed (0.4 Mach), and solid-particle erosion conditions. Yttria-stabilized zirconia (YSZ) TBCs were prepared using electron beam physical vapor deposition (EB-PVD). For different erosion durations (2 h, 5 h, 8 h, 12 h), the evolution of macroscopic and microscopic morphologies as well as the development of residual stresses in the thermally grown oxide (TGO) layer were systematically investigated. The results indicate that the erosion process of the YSZ coating can be divided into three stages. During the initial high-erosion-rate stage (8.17 g/kg), erosion damage was confined to the grain tips of the columnar crystals, primarily caused by brittle fracture at the grain tips, and the TGO stress was relatively low (−0.6 GPa). During the intermediate stage, the erosion rate was lower (2.74 g/kg). Impact stresses induced microcracks within the columnar grains, which gradually connected to form intergranular fractures. This led to the expansion of localized spalling pits. The interface began to wrinkle, and the stress rose to −2.2 GPa. In the final accelerated failure stage (5.88 g/kg), horizontal cracks fully propagated, leading to large-scale peeling of the coating. The stress was released to −0.9 GPa. The coating failure mechanism evolves from surface damage to interfacial peeling, which is closely related to the coating structure, stress evolution, and interfacial state.

Förderung

  • Beijing Institute of Aeronautical Materials

Zitieren

APA

Yang, W., Mu, R., He, L., Li, S., Cai, H., & Liu, D. (2026). Failure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment. Coatings, 16(5), 574. https://doi.org/10.3390/coatings16050574

Vancouver

Yang W, Mu R, He L, Li S, Cai H, Liu D. Failure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment. Coatings. 2026;16(5):574. doi:10.3390/coatings16050574

BibTeX
@article{Yang2026,
  author = {Yang, Wenhui and Mu, Rende and He, Limin and Li, Shuai and Cai, Huangyue and Liu, Delin},
  title = {Failure Mechanisms of EB-PVD Thermal Barrier Coating in Simulated Aero-Engine Erosion Environment},
  journal = {Coatings},
  year = {2026},
  volume = {16},
  number = {5},
  pages = {574},
  doi = {10.3390/coatings16050574}
}
Kostenlos starten →