Investigation of Tool Wear and Surface Integrity in Turning γ-TiAl Alloy Under High-Pressure Cooling
Coatings · 03.04.2026 · 16 (4) · 428
DOI: 10.3390/coatings16040428 ↗Kurz gefasst
Fachartikel in der Zeitschrift Coatings, online erschienen am 03.04.2026. Verfasst von Erliang Liu und 4 weiteren Autor:innen. Die Arbeit wurde bisher 3-mal zitiert (Crossref) und nennt 38 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Jiangsu Province, Gansu Provincial Natural Science Foundation.
Abstract (Originalsprache)
To address the issues of high cutting temperature and insufficient heat dissipation during the machining of γ-TiAl alloys, this study systematically investigates the effects of three cooling strategies—dry cutting, flood cooling, and high-pressure cooling—on tool wear and surface integrity. The variations in tool wear, surface morphology, surface roughness, surface defects, microstructure, and microhardness were analyzed in detail. The experimental results indicate that adhesive wear is the dominant wear mechanism under all three cooling conditions. Owing to its superior penetration capability, high-pressure cooling significantly suppresses tool wear, although it may induce groove wear. In terms of surface integrity, high-pressure cooling significantly improves the machined surface quality while reducing surface defects, plastic deformation, and work hardening. Compared with dry cutting, the surface roughness decreases by approximately 9.1%–39.0%, the thickness of the plastically deformed layer is reduced by up to 50.74%, and the degree of work hardening decreases by approximately 11.5%–14.5%. With increasing cutting speed, the surface roughness, plastically deformed layer thickness, and degree of work hardening increase under all three cooling conditions; however, high-pressure cooling still maintains the best overall performance at high cutting speeds. These results indicate that high-pressure cooling effectively suppresses thermo-mechanical coupling in the cutting zone by enhancing coolant penetration and lubrication, thereby providing an efficient approach to reducing tool wear and improving the surface quality of machined γ-TiAl alloys.
Förderung
- National Natural Science Foundation of China
- Natural Science Foundation of Jiangsu Province
- Gansu Provincial Natural Science Foundation
Zitieren
APA
Liu, E., Xu, Y., Zhu, B., Shi, L., & Zhou, H. (2026). Investigation of Tool Wear and Surface Integrity in Turning γ-TiAl Alloy Under High-Pressure Cooling. Coatings, 16(4), 428. https://doi.org/10.3390/coatings16040428
Vancouver
Liu E, Xu Y, Zhu B, Shi L, Zhou H. Investigation of Tool Wear and Surface Integrity in Turning γ-TiAl Alloy Under High-Pressure Cooling. Coatings. 2026;16(4):428. doi:10.3390/coatings16040428
BibTeX
@article{Liu2026,
author = {Liu, Erliang and Xu, Yifan and Zhu, Baiwei and Shi, Limin and Zhou, Hailang},
title = {Investigation of Tool Wear and Surface Integrity in Turning γ-TiAl Alloy Under High-Pressure Cooling},
journal = {Coatings},
year = {2026},
volume = {16},
number = {4},
pages = {428},
doi = {10.3390/coatings16040428}
}
EUVIMED