EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Skid Resistance Attenuation of Asphalt Pavement Based on Multifactor Accelerated Wear Test

Lujie Qi, Yamin Liu, Zhongliang Liu, Congcong Zhang, Zhenshan Chen, Jin Lv, Haifeng Wan

Coatings · 31.03.2023 · 13 (4) · 717

DOI: 10.3390/coatings13040717 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Coatings, online erschienen am 31.03.2023. Verfasst von Lujie Qi und 6 weiteren Autor:innen. Die Arbeit wurde bisher 11-mal zitiert (Crossref) und nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Shaanxi Province, Transportation Science and Technology Project of Shandong Province.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To describe the skid resistance attenuation of asphalt pavement during its life cycle, this paper selected a multi-variable accelerated abrasion machine to simulate the abrasion process, and British Pendulum Number was selected to evaluate the skid resistance after various abrasive cycles. During the abrasion process, three factors influencing the skid resistance were considered, including aggregate types (diorite, limestone, granite, and basalt), nominal maximum aggregate size (NMAS), and gradations (dense, gap, and open). The results show that with increasing abrasion cycles, the skid resistance of asphalt pavement firstly decreases rapidly in the first abrasion stage (0–8000 cycles), then at a relatively gentle rate in the second abrasion stage (8000–20,000 cycles), and finally at the lowest rate in the third abrasion stage (after 20,000 cycles). The skid-resistance durability and stability of pavement are ranked as basalt > granite > amphibolite > limestone. Moreover, the effect of aggregate parameters on skid resistance is in the order: angularity > PSV > WSV > CSV. The skid resistance and its stability improve as NMAS increases. The pavement skid durability is in the order: SMA > OGFC > AC. In addition, the sizes of 16 mm, 13.2 mm, 9.5 mm, 0.6 mm, 0.3 mm and 0.15 mm are the critical sieve sizes to improve the skid resistance of asphalt pavement.

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Shaanxi Province
  • Transportation Science and Technology Project of Shandong Province
  • research project of Transportation Department of Fujian Province of China
  • Transportation Technology Project of Shandong Province

Zitieren

APA

Qi, L., Liu, Y., Liu, Z., Zhang, C., Chen, Z., Lv, J., & Wan, H. (2023). Skid Resistance Attenuation of Asphalt Pavement Based on Multifactor Accelerated Wear Test. Coatings, 13(4), 717. https://doi.org/10.3390/coatings13040717

Vancouver

Qi L, Liu Y, Liu Z, Zhang C, Chen Z, Lv J, et al. Skid Resistance Attenuation of Asphalt Pavement Based on Multifactor Accelerated Wear Test. Coatings. 2023;13(4):717. doi:10.3390/coatings13040717

BibTeX
@article{Qi2023,
  author = {Qi, Lujie and Liu, Yamin and Liu, Zhongliang and Zhang, Congcong and Chen, Zhenshan and Lv, Jin and Wan, Haifeng},
  title = {Skid Resistance Attenuation of Asphalt Pavement Based on Multifactor Accelerated Wear Test},
  journal = {Coatings},
  year = {2023},
  volume = {13},
  number = {4},
  pages = {717},
  doi = {10.3390/coatings13040717}
}
Kostenlos starten →