EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Sulfur Dispersant Coverage Constraints and Corrosion Monitoring for Sour Gas Gathering Systems

Yunxia Lan, Changqing Jia, Yun Jiang, Xiang Chen, Peitao Liu, Kun Zhao, Ruowen Yu, Shuai Deng, Guoxi He

Corrosion and Materials Degradation · 29.10.2026 · 7 (4) · 72

DOI: 10.3390/cmd7040072 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Corrosion and Materials Degradation, online erschienen am 29.10.2026. Verfasst von Yunxia Lan und 8 weiteren Autor:innen. Die Arbeit nennt 30 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Startup delays can leave sulfur-deposit-prone gathering nodes below a prescribed dispersant concentration despite adequate steady dosing. This study combines archived characterization, a conditional experimental mixing comparison and transport calculations for sour gas-gathering systems. Active-flux conservation, route retention and delayed startup response yield finite-deadline dose bounds and a coverage deficit integral (CDI). Twenty solids show local sulfur fractions of 3.71–58.00 wt.%, and 11 of 13 diffraction patterns match orthorhombic S8. Six calendar-date water pairs show total-sulfur ratios of 8.20–47.96, interpreted descriptively. Six chloride/bromide comparisons from formulation–water blends deviate by −11.1 to +0.7% from an unfitted ideal-dilution benchmark. This check assumes additive volumes, a volume-concentration basis and zero formulation background. Under prescribed transport conditions, 12 h coverage requires 28.84 L/d at nominal inputs and 63.30 L/d over the rectangular parameter set. A 60 L/d cap reaches the illustrative 50 mg/L threshold after 13.00 h in the worst combination. Variable-flow and reversible-storage alternatives test structural sensitivity. CDI summarizes delivery shortfall without establishing a damage response. The experimental comparison concerns conservative ion mixing; field dosing and corrosion predictions require separate active-residual and material-response calibration.

Zitieren

APA

Lan, Y., Jia, C., Jiang, Y., Chen, X., Liu, P., Zhao, K., Yu, R., Deng, S., & He, G. (2026). Sulfur Dispersant Coverage Constraints and Corrosion Monitoring for Sour Gas Gathering Systems. Corrosion and Materials Degradation, 7(4), 72. https://doi.org/10.3390/cmd7040072

Vancouver

Lan Y, Jia C, Jiang Y, Chen X, Liu P, Zhao K, et al. Sulfur Dispersant Coverage Constraints and Corrosion Monitoring for Sour Gas Gathering Systems. Corrosion and Materials Degradation. 2026;7(4):72. doi:10.3390/cmd7040072

BibTeX
@article{Lan2026,
  author = {Lan, Yunxia and Jia, Changqing and Jiang, Yun and Chen, Xiang and Liu, Peitao and Zhao, Kun and Yu, Ruowen and Deng, Shuai and He, Guoxi},
  title = {Sulfur Dispersant Coverage Constraints and Corrosion Monitoring for Sour Gas Gathering Systems},
  journal = {Corrosion and Materials Degradation},
  year = {2026},
  volume = {7},
  number = {4},
  pages = {72},
  doi = {10.3390/cmd7040072}
}
Kostenlos starten →